I can't find any woven wire cloth locally. Does anyone know of anyplace that carries such a thing? Online or mail order? I'm attempting a fireplace screen.
Reply With Quote
  #2  
Old 09-24-2005, 12:04 PM
Ries Ries is offline
WeldingWeb Foreman
 
Join Date: May 2004
Location: Edison Wa.
Posts: 695
Easiest place to get it is McNichols-
http://www.mcnichols.com/

They have warehouses all over the country, and they will ship to anyone- ups for small stuff, or a 40 foot semi if thats what you want.

They are NOT the cheapest place- but they have everything, including the wierd stuff you cant find anywhere else- I just ended up buying a bunch of stainless 2" square wire mesh from them, in 4x10 sheets- cause where the hell else are you gonna get it?
Reply With Quote
  #3  
Old 09-24-2005, 06:53 PM
Nick Kent Nick Kent is offline
WeldingWeb Journeyman
 
Join Date: Jan 2005
Location: Cape Ann area, MA
Posts: 152
Thanks very much.
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 03:19 PM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.