greetings

I'm a fabricator and student from New Mexico. At work I run a lot of 1/8" 7018 on a gas driven welder (Bluestar 185 DX and a little Hobart) and dual shield .045" on a Millermatic 252
__________________
Power of Blue Baby!
Reply With Quote
  #2  
Old 08-30-2009, 01:42 PM
specter's Avatar
specter specter is offline
Master Welder
 
Join Date: Aug 2008
Location: Dansville NY
Posts: 5,185
Re: greetings

Hi Ya Blutrane and Welcome to the Welding Web Family. What kind of stuff do you fabricate?
__________________
Co-Own CNC shop:Miller :1251 plasma cutter, MaxStar 700 TIG/Stick, & XMT 456 Multiprocess Welder.& 2 Hypertherm HPR260's Plasma Cutter

Sorry I had a bad stroke but now I am back.
Reply With Quote
  #3  
Old 08-30-2009, 09:45 PM
Blutrane's Avatar
Blutrane Blutrane is offline
Solderer
 
Join Date: Aug 2009
Location: Albuquerque, NM
Posts: 9
Re: greetings

a "FASTek" a machine for loading shipping containers with steel scrap
__________________
Power of Blue Baby!
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 01:23 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.