HF Compact Bender Projects
Questions for you-all. Anyone know of a list of compact bender projects? Maybe a book ar a video would be nice. I've used mine to make scrolls and a Monte Carlo brace , but most of the time it just sits there collecting dust. Thats a shame ... help if you can.
|
|
#2
|
|||
|
|||
|
I went to Hossfeld's website. They show many ways to use the bender. I do stock lambs tongues for handrails--got this idea from the Hossfeld website. I can crank lots of them out is short amount of time.
Tried to sell mine once, glad I didn't... comes in handy when I have a lot of repeat bends. Took a long time to figure out how to use it. I'd be interested in hearing what others do with their benders, too. |
|
#3
|
|||
|
|||
|
My HF bender is painted a glossy rich RED, I have anchor bolts inside my shop and out in the driveway(for more room), and at best can make a few simple rt angle bends. I need a video, BAD!!
|
|
#4
|
|||
|
|||
|
www.toolsplus1.com/compactbend.htm for video. Also search the archives of this message board.
|
|
#5
|
|||
|
|||
|
I am also looking for an instructional video. I found this http://www.ironprojects.com/video1.htm
It's 29.95 VHS or DVD. I plan to order one and check it out |
|
#6
|
|||
|
|||
|
Quote:
|
|
#7
|
|||
|
|||
|
lurkin'
|
|
#8
|
|||
|
|||
|
Manual Link
They have upgraded the manual pics. Here is a link to the new manual. At quick glance it looks pretty **** good.