#1
|
|||
|
|||
|
Pro Arc 200
Hello
Just ordered a Pro Arc 200 I am looking forward to using this 200 amp inverter,I have heard good things about Everlast.I own and use a lot of welding equip and just sent in My TA 185 for repairs (out of warranty) and expect the repair bill to be more than the cost of the Pro arc 200, I have used my Riland 60 plasma for 4-5 years now and the only regret I have is that I did not get a 80 amp machine (not available at the time) My diesel welder (Chinese) has done a lot of welding 5 years flawless. I have had a Lincoln and Hobart die on me Now my Ta 185 so I can say everything gives up the ghost sometimes. I think Jefftrent is just bashing Everlast he probably don't know which end of the stick to put in the holder if truth be known! Bobs Welding Fillmore NY
__________________
Thermal Arc T-Bird 270 Amp gas welder Thermal Arc Pro Wave 185 PowerArc 200 Riland 60 Plasma Miller suitcase 12vs wire feeder, 180 Amp Diesel Welder Gen Ellis 1600 bandsaw Imig 205 Mig,Century GS170 Mig Lincoln 250 G9 Pro gas Weldanpower Last edited by doxie; 09-08-2010 at 08:33 PM. Reason: spelling |
|
#2
|
||||
|
||||
|
Re: Pro Arc 200
Hi,
Doxie, Did you mean PowerARC 200? Its a good machine. It has a stable arc and spatter is ridiculously low.
__________________
Welders: Esab Migmaster 250 Penncraft 230 (oldy but goody) HF Plasma 30 (Italian) Lincoln Ranger 8 Smith Oxy/Acetylene/Propane Lincoln SA200 Everlast Power Tig 250 EX Everlast PowerUltra 205 |
|
#3
|
|||
|
|||
|
Re: Pro Arc 200
Yes it is a PowerArc 200 ,I will edit my post.
Thanks Bob Well I can not edit orig post ,maybe a moderator can change the words pro arc 200 to PowerArc 200 in my org.post Thanks Bob
__________________
Thermal Arc T-Bird 270 Amp gas welder Thermal Arc Pro Wave 185 PowerArc 200 Riland 60 Plasma Miller suitcase 12vs wire feeder, 180 Amp Diesel Welder Gen Ellis 1600 bandsaw Imig 205 Mig,Century GS170 Mig Lincoln 250 G9 Pro gas Weldanpower Last edited by doxie; 09-08-2010 at 09:50 PM. |
|
#4
|
|||
|
|||
|
Re: Pro Arc 200
I've been using the PowerArc 200 for about a month. It is a very efficient and effective DC welder.
As Mark stated - stable arc, very little splatter, quick starts and restarts, smooth and quiet. Much more refined than my transformer Lincoln AC/DC tombstone. |
![]() |