Lincoln buzzbox upgrade's
I've decided to do a little upgrading to my lincoln AC225 buzzbox.I went by my local tractor supply to look at their welding accessories plus I had a 10 dollar off coupon so I purchased a hobart 400 amp brass ground clamp to start the upgrade.It is sold by hobart but is made in china,what a disappointment,as you can see it has hobart nowhere but china is cast into the brass,but hey,had a 10 dollar off coupon so it went from $19.99 down to $9.99.I am going to take the welder all apart and clean it up and give it a fresh coat of paint.I've had this welder forever and it still works like a champ but hardly ever gets used but is always there when I need it for some serious amps.Will probably get a new stinger next.I will try and take some pics along the way..............doug
__________________
Maxus Pro-125 Mig Chicago Electric 90 amp DC flux-core Lincoln Electric AC 225 tombstone O/A torch M/O mini-torch 10 acres of flatland 15 acres of holler Last edited by dugndeep; 10-06-2010 at 10:41 PM. Reason: more |
|
#2
|
||||
|
||||
|
Re: Lincoln buzzbox upgrade's
that is a nice ground clamp you got there.
I've been thinking of grabbing an old ground cable from a car, stripping the wire, and looping it inside my cheapo clamp. I think it will make a big difference. |
|
#3
|
||||
|
||||
|
Re: Lincoln buzzbox upgrade's
Taiden-I think it would too.I bought a lincoln ground clamp with the copper shunt and could tell a big difference compared to the original ground clamp on my chicago electric 90 amp flux core welder.