#1  
Old 05-04-2011, 07:47 PM
russ69coupe's Avatar
russ69coupe russ69coupe is offline
WeldingWeb Journeyman
 
Join Date: Jan 2007
Location: Warren, Ohio
Posts: 82
Does all chrome moly tubing need to be Tig'd?

Looking at a mounting kit for a fiberglass front end on my current project car. Problem is it is made out of chrome moly. Don't have the size/gauge of the tubing, but it is smaller than roll bar stuff.
Thanks,
Russ
__________________
RIP Mallory, we miss you.
Reply With Quote
  #2  
Old 05-04-2011, 07:51 PM
zapster's Avatar
zapster zapster is offline
Moderator
 
Join Date: Jan 2006
Location: In A Nice Comfy Chair
Posts: 13,812
Re: Does all chrome moly tubing need to be Tig'd?

Tig is your best bet but Mig can be used...
No Fluxcore..

...zap!
__________________


I am not completely insane..
Some parts are missing

I have figured out that keeping everyone happy is nearly impossible but pissing people off is easy and fun.
Reply With Quote
  #3  
Old 05-04-2011, 10:03 PM
norite norite is offline
WeldingWeb Foreman
 
Join Date: Aug 2008
Location: Sudbury, Ontario
Posts: 589
Re: Does all chrome moly tubing need to be Tig'd?

x2 what zapster said

Also oxy-acetylene is often used for building aircraft with c-m tubing..
__________________
"The reason we are here is that we are not all there"

SA 200
Idealarc 250 AC DC
MM200
MM251
30a Spoolgun & WC24 Control
Square Wave Tig 175
Invertec V350 Pro
SC-32 CS 12 Wire Feeder
Oxweld/Purox O/A
ArcAir gouging torch
Need Plasma
Reply With Quote
  #4  
Old 05-05-2011, 11:29 AM
fortyonethirty fortyonethirty is offline
WeldingWeb Foreman
 
Join Date: May 2009
Location: San Luis Obispo, CA
Posts: 749
Re: Does all chrome moly tubing need to be Tig'd?

I would not pass up the opprtunity to TIG some 4130. Chromoly welds so nice I'd tig it just for fun. But, no you you don't have to tig it.
__________________
Ian Tanner

Kawasaki KX450f and many other fine tools

Last edited by fortyonethirty; 05-05-2011 at 11:36 AM.
Reply With Quote
  #5  
Old 05-05-2011, 01:24 PM
Donald Branscom's Avatar
Donald Branscom Donald Branscom is offline
WeldingWeb Craftsman
 
Join Date: Dec 2007
Location: Guerneville Ca
Posts: 1,682
Re: Does all chrome moly tubing need to be Tig'd?

How thin IS the tubing?
__________________
AWS certified welding inspector
AWS certified welder
44 years experience.
Miller 110V 140 MIG
Miller Elite auto sensing helmet.
Reply With Quote
  #6  
Old 05-05-2011, 02:24 PM
Pangea Pangea is offline
WeldingWeb Tradesman
 
Join Date: Feb 2011
Location: Tennessee
Posts: 272
Re: Does all chrome moly tubing need to be Tig'd?

I welded lots of 4130 high pressure pipe for oil field use with MIG and Spray Arc. Pre heat to about 500 and use ER70S wire.
__________________
Two turn tables and a microphone.
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 01:02 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.