| Register | FAQ | Members List | Calendar | Search | Today's Posts | Mark Forums Read |
![]() |
|
|
Thread Tools | Display Modes |
|
#1
|
|||
|
|||
|
How can GTAW be legal?
It is way too much fun!!!
I just got a bottle for my new Syncrowave 200 yesterday and fired it up. It is awesome! Not like I know what I am doing or anything but this is some fun $hit! The amount of control you have is amazing, just watching the arc form, the puddle form, then solidify back as you play with the peddle and the reaction the metal has in and around the puddle. You guys have been keeping this TIG stuff a secret from us down and dirty MIG weld guys. Sure MIG is easy and fast, but this TIG stuff is the cat's a$$! My $0.02. |
|
#2
|
||||
|
||||
|
Re: How can GTAW be legal?
And you know, I thought I was the only person in the world that gets this excited about GTAW welding. Seriously. I probably stick weld 5 times more than I do GTAW and I love that too but there's something extremely cool about this process. I just got done running some this afternoon on a lid I'm making for a tongue box in the front of an HE trailer. Just some steel diamond plate to a frame but I wanted it to have that signature TIG look so I took the time to run it this way.
I love it! Glad you do too. Enjoy. E |
|
#3
|
|||
|
|||
|
Re: How can GTAW be legal?
SSSHHHHHHHHH! Quit talking about it unless you want to see a tax put on it!
__________________
"Stick-man is wise" - Farmall "Stick-man is right. Much as it pains me to admit it, the thieving knucklehead." tbone550 "StickyFingers-man" Commander 500D, LN25 Shopmaster 300, Super S-32P Hypertherm Pmax 600 Smith & Oxweld O/P |
|
#4
|
|||
|
|||
|
Re: How can GTAW be legal?
Their getting ready to outlaw it.
__________________
Miller Synchro250 bought new 1997 Millermatic200 Miller Bluestar 2E . AC/DC 16hp Bluestar 2E , DC Miller Thunderbolt225 AC/DC Arc Longevity 60 plasma |
|
#5
|
|||
|
|||
|
Re: How can GTAW be legal?
They will get mine when they pry it from my cold dead fingers!
![]() Thurmond
__________________
Miller Bobcat 3 Phase, 26 series gas cooled TIG torch Miller Suitcase X-Treme 12VS 17 Series Tig Torch for Solar Panel Powered Welding Oxy/Acetylene Torch rig EVERLAST PowerUltra 205P |
|
#6
|
|||
|
|||
|
Re: How can GTAW be legal?
Quote:
__________________
Ian Tanner Kawasaki KX450f and many other fine tools Last edited by fortyonethirty; 08-14-2011 at 07:50 PM. |
|
#7
|
||||
|
||||
|
Re: How can GTAW be legal?
I was jassed like that when I tried DC tig on my powcon and foun out how well it worked for a basic scratch start machine. The arc being so precise and having such a great puddle view do make it a fun process to use
__________________
Airco 330A/BP. Lincoln SP250 W/ spoolgun, GoWeld x2 TA Predator, ESAB 300AVS Feeder ESAB 875 plasma. . Bernard Cooler. Evo 355. OA Demo: Longevity Tigweld 200SX, Forcecut 42i Everlast 140ST.. On loan to friend/sale pending Last edited by soutthpaw; 08-14-2011 at 08:08 PM. |
|
#8
|
||||
|
||||
|
Re: How can GTAW be legal?
hmmm, just got back from work, got 4-5 hours arc time... I'll ask for more tomorrow ...
)
|
|
#9
|
||||
|
||||
|
Re: How can GTAW be legal?
You guys have NO idea what you are getting yourself into..
![]() ...zap!
__________________
![]() I am not completely insane.. Some parts are missing ![]() I have figured out that keeping everyone happy is nearly impossible but pissing people off is easy and fun. |
|
#10
|
||||
|
||||
|
Re: How can GTAW be legal?
C'mon Zap,
You know you love it too. I've seen some of your work. Anyone that TIGs like you do has to love it. Besides, you get ALL the fun jobs. E |
|
#11
|
||||
|
||||
|
Re: How can GTAW be legal?
I have found tig to be almost better than sex, , , cornemuse
|
|
#12
|
|||
|
|||
|
Re: How can GTAW be legal?
It is really, really fun. MIG is great functionally. I don't have the skill or money to buy a great MIG welder to do the whole "mig like tig" pretty weld thing, so to me TIG is like using a brush and MIG is like using a can of spray paint. It truly is fun.
|
|
#13
|
|||
|
|||
|
Re: How can GTAW be legal?
try shortening arc length..
|
|
#14
|
|||
|
|||
|
Re: How can GTAW be legal?
o p , sounds like you'd enjoy gas welding too...
|
|
#15
|
|||
|
|||
|
Re: How can GTAW be legal?
I told my wife the same thing, she told me "you must be doing it wrong", didn't ask her to eaborate as to which she was referring to.--Matt
__________________
4 Miller Big Blue 600 Air Paks 2 Miller 400D 6 Lincoln LN-25's 4 Miller Xtreme 12VS 4 Miller XMT 350's 8 Miller Pro-300D 4 Climax BW-3000Z bore welders 4 T D Pro-152's Miller Dynasty 350 3 Linc DC-600 1 Linc 500-I Pair of Welpers |
|
#16
|
||||
|
||||
|
Re: How can GTAW be legal?
I've always loved the way the beads look nothing like some good old weld porn to look at.
__________________
Will Supports Autism AwarenessMy Toys BobCat 225 PLus Millermatic 130 Miller Spectrum 300 Cutmate Everlast Power Tig 185 Micro April is Autism Month . |
|
#17
|
||||
|
||||
|
Re: How can GTAW be legal?
I don't know about that but its a close second
__________________
Will Supports Autism AwarenessMy Toys BobCat 225 PLus Millermatic 130 Miller Spectrum 300 Cutmate Everlast Power Tig 185 Micro April is Autism Month . |
|
#18
|
||||
|
||||
|
Re: How can GTAW be legal?
Try combining both these activities together at the same time, it will really blow your mind, as well as something else.
![]()
|
|
#19
|
||||
|
||||
|
Re: How can GTAW be legal?
Im just in it for the burning metal smell
__________________
SQUARE WAVE 175 TIG DUAL MIG 151
|
|
#20
|
|||
|
|||
|
Re: How can GTAW be legal?
Quote:
|
|
#21
|
|||
|
|||
|
Re: How can GTAW be legal?
Better than sex....no
Fun....yea. I just like how quiet and clean it is (especially on DC)...there's no crackle pop and sparks flying all over, just nice and tidy. |
|
#22
|
||||
|
||||
|
Re: How can GTAW be legal?
im with you guys this is way to much fun and if you call it work your crazy i would almost weld for free LOL.
|
|
#23
|
||||
|
||||
|
Re: How can GTAW be legal?
DLite said
"Better than sex....no" I said "ALMOST", , , , better, , -corne- (edit) He also said: "I just like how quiet and clean it is (especially on DC)...there's no crackle pop and sparks flying all over, just nice and tidy." I thought welders do it in ALL positions haha -c- Last edited by cornemuse; 04-24-2012 at 10:07 AM. |
|
#24
|
|||
|
|||
|
Re: How can GTAW be legal?
Quote:
Some positions are more fun than others!!
|
|
#25
|
||||
|
||||
|
Re: How can GTAW be legal?
I don't know about that, having to do it every day 8-10 hours may take the fun out of it.
__________________
Will Supports Autism AwarenessMy Toys BobCat 225 PLus Millermatic 130 Miller Spectrum 300 Cutmate Everlast Power Tig 185 Micro April is Autism Month . |
![]() |