target stands

Made 8 of these for work the other day. The county purchased the extreamly rusty steel 1/8 1-1/2 angle and 1/8 2" sq tube. The stands are not pretty but they are target stands not space shuttle parts. The angle on the front of the tube will prevent the tubing from being dented in and pinching the wooden furing strips in the tube when hit from handgun rounds.

Name:  target stand 1.jpg
Views: 670
Size:  41.5 KB

Name:  stands 3.jpg
Views: 664
Size:  69.6 KB

Name:  stands 5.jpg
Views: 661
Size:  46.6 KB

Last edited by BRICKmp5; 08-01-2006 at 03:34 AM. Reason: spelling mistake
Reply With Quote
  #2  
Old 08-01-2006, 03:24 AM
MAC702's Avatar
MAC702 MAC702 is offline
WeldingWeb Artisan
 
Join Date: Jan 2004
Location: Las Vegas, NV
Posts: 3,188
Re: taget stands

Man, I made a ton of those when I was shooting IPSC every weekend. Nice job!
Reply With Quote
  #3  
Old 08-01-2006, 03:28 AM
BRICKmp5 BRICKmp5 is offline
WeldingWeb Apprentice
 
Join Date: Apr 2006
Location: Ohio
Posts: 21
Re: taget stands

thanks, I think i made submitted two threads when I attempted to correct my spelling mistake. whoops still trying to figure all this out.
Reply With Quote
  #4  
Old 08-01-2006, 10:36 PM
Sandy Sandy is offline
Master Welder
 
Join Date: Jan 2004
Location: Northern Cal., Shasta County
Posts: 4,786
Re: target stands

Good job. So the wooden frame material is some standard cut like the so called 2X2's or similar?? Something similar might work good for the occasional rifle sighting in. Not much there to store once you take the 2X2 out.
Reply With Quote
  #5  
Old 08-02-2006, 03:08 AM
BRICKmp5 BRICKmp5 is offline
WeldingWeb Apprentice
 
Join Date: Apr 2006
Location: Ohio
Posts: 21
Re: target stands

Sandy, we buy 2x2 furing strips by the bundle because they get shot up quite a bit during qualification and firearms training. When the wood posts are out they are pretty easy to store and don't take up too much space. I made the base 25" wide because it matches the dimensions for the bulk cardboard used as the target backer. They legs are 36" long each so the wind doesn't knock them over. I bet you could make a set of these with folding legs so they take up even less space.
Reply With Quote
  #6  
Old 08-02-2006, 05:32 PM
fwalz3's Avatar
fwalz3 fwalz3 is offline
WeldingWeb Journeyman
 
Join Date: Mar 2006
Location: Somewhere in NJ
Posts: 195
Re: target stands

That's an interesting idea. We use a wooden frame to hold the cardboard and target and then use wire to hang it on a cable that runs in front of the backstop. Works well except on a windy day, the targets tend to swing back and forth which makes it a little more challenging. Your idea looks much more stable.
__________________
Sure, I can fix it... I got a welder!!!
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 07:06 PM.


Powered by vBulletin® Version 3.8.1
Copyright ©2000 - 2010, Jelsoft Enterprises Ltd.
Copyright ©2000 - 2009, Penton Media, Inc. All rights reserved.