A little SS repair..

I have to repair some cracks in two SS truck fenders...
Attached Images
     
__________________
Lincoln pro mig 180
Lincoln Square Wave Tig 300/wp 20/home built water cooler
Victor, Purox, Harris, O/A welding/cutting setups
Vintage Craftsman drill press
Vintage Craftsman/Atlas 12"x 36'' lathe
7''x 12'' w/c band saw
Everlast 140 st
Reply With Quote
  #2  
Old 01-29-2012, 06:27 PM
DemonSpeeder's Avatar
DemonSpeeder DemonSpeeder is offline
WeldingWeb Craftsman
 
Join Date: Jul 2011
Location: North,Ga
Posts: 1,036
Re: A little SS repair..

......
Attached Images
 
__________________
Lincoln pro mig 180
Lincoln Square Wave Tig 300/wp 20/home built water cooler
Victor, Purox, Harris, O/A welding/cutting setups
Vintage Craftsman drill press
Vintage Craftsman/Atlas 12"x 36'' lathe
7''x 12'' w/c band saw
Everlast 140 st
Reply With Quote
  #3  
Old 01-30-2012, 06:52 AM
David R's Avatar
David R David R is offline
Master Welder
 
Join Date: Feb 2007
Location: West By Golly Shelby NY
Posts: 7,246
Re: A little SS repair..

Tractor trailer? Milk Hauler?

You gonna polish them out?

David
__________________
Real world weldin.

When I grow up I want to be a tig weldor.
Reply With Quote
  #4  
Old 01-30-2012, 06:18 PM
DemonSpeeder's Avatar
DemonSpeeder DemonSpeeder is offline
WeldingWeb Craftsman
 
Join Date: Jul 2011
Location: North,Ga
Posts: 1,036
Re: A little SS repair..

Tractor trailer (over the duals), I'm going to try to polish them, but for now he just wants to get them fixed and mounted, Also this was my first time using my new(to me) Square Wave tig. The pedal isn't as responsive as the Precision tig I have been using in school...
__________________
Lincoln pro mig 180
Lincoln Square Wave Tig 300/wp 20/home built water cooler
Victor, Purox, Harris, O/A welding/cutting setups
Vintage Craftsman drill press
Vintage Craftsman/Atlas 12"x 36'' lathe
7''x 12'' w/c band saw
Everlast 140 st
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 05:25 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.