Looking at a wire feeder by hobart mdl # 5687 V5. unit has push- pull on gun

does anyone know anything about this unit. says it will work on cc and cv

just wondering

thanks:waving:

Cruizer
03-10-2008, 11:11 AM
Only voltage sensing feeders will work in CC!!!

Otherwise CV is your only choice