I purchased a set 3. 6" 12" 18" and find them to be quite less than I expected. All three are the same. The hooks on one side don't sit flush from either poor parts or poor workmanship, the corners of the scale have burrs and the ends are cut crooked to boot. I was wondering if anyone else has them and what they think. I don't find it too difficult to measure within a few thousandths with a scale but that is not going to happen with these things and I wish I would have looked for some used gear on ebay instead.

jpump5
03-29-2016, 05:41 PM
I was considering one of those. Now I'm glad I didn't go for it.
Bought an 18" rule from Enco when member BD1 posted
about sale.

mikecwik
03-29-2016, 05:50 PM
I like PEC very much. Nice quality for the money. TaylortoolworksIIc is where I got the Igaging on Ebay and he has what looks to be nice prices on PEC's