Any comments on the pro core 100? It says it will weld 1/4'', I can get a pretty good deal on one right now. Anything you guys have would be appreciated. thanks

redfish_joe
11-07-2006, 10:23 PM
I have one and well pleased with it. Just made a fish cooker/crab boiler with it. Made a burner guard out of 3/8" flat stock and it welded the p##s out of it. :cool: