Whipped up a tungsten grinding holder for about $15.00 (drill bit and Dremel keyless chuck) had some round stock laying around.

https://youtu.be/4DJYNdS3Sik

ironmangq
10-07-2016, 02:31 PM
Pin vices are cheap and can work too, might not have the depth though.

jpitz31
10-11-2016, 01:58 PM
Changed the copyrighted music, Here is new link


Deleted per the 40 post rule...

Sorry but this is how the game is played.

...zap!

oldgrandad
10-24-2016, 05:58 PM
I put this together from harbor freight the grinder was $35 and I got the replacement saw blade sharpening set #98862 for $10 153383115338411533851

jagboy69
10-27-2016, 09:43 PM
WTF is the 40 post rule????

strokedbronco
10-28-2016, 09:32 AM
I'm pretty sure it's that you can't post videos until you have at least 40 posts....I'm sure one of the mods can help explain or you can find it in the "rule book." It's to help prevent people from signing up just to spam this wonderful forum!

soutthpaw
10-28-2016, 01:01 PM
Been using the same saw sharpening disc on my 3" HF grinder for years

Billdacat
10-29-2016, 08:08 AM
I was thinking of getting a really cheep HF grinder to poke 7018 rod's into with one hand.

John T
10-29-2016, 08:38 AM
seems everyone has their own ideas for tungsten sharpening.
I've tried the diamond wheel on bench grinder and belt sander methods,

but finally sprung for a tech south...

WELL worth the money IMO.

quick, simple and accurate. you can adjust it however you want for any size.
most guys spend thousands of dollars on welding machines then piss and moan they can't afford a couple hundred for a dedicated sharpener...