Welding Fail! post pics here. - Page 84
RSS | Subscribe | Contact Us | Advertise | About Us
Page 84 of 86 FirstFirst ... 34748283848586 LastLast
Results 2,076 to 2,100 of 2132
  1. #2076
    Join Date
    Jan 2016
    Posts
    2,791

    Re: Welding Fail! post pics here.

    Quote Originally Posted by motolife313 View Post
    Thanks for the words of advise hobbytime, learning from your mistakes is the best way to learn. And this was a little mistake lol
    your 100% correct, as long as the mistake doesnt kill you..then you dont have to worry about it...

  2. #2077
    Join Date
    Mar 2006
    Location
    Yuma, Arizona
    Posts
    3,349

    Re: Welding Fail! post pics here.

    Why has he not been banned yet? Agreed, douche.
    Lincoln Power Mig 350MP - MIG and Push-Pull
    Lincoln Precision TIG 275,Undercart cooler,Foot/Finger Amptrollers
    Lincoln Hobby-Weld 110v
    Lincoln SP-200 MIG and Hi-Freq Tig
    CK TIG TORCH, gas diffuser, pyrex cup
    Thermal Dynamics Cutmaster 101

  3. #2078
    Join Date
    Feb 2016
    Location
    East Texas
    Posts
    386

    Re: Welding Fail! post pics here.

    There is a little run of pipe fence with some terrible welds, next to one of the fences I am working on. I will have to get a video, because it it easier than uploading pictures.
    Forney C5 Arc Welder
    Lincoln Idealarc 250-250 Ac/Dc Arc Welder
    Miller Bobcat 225g Plus
    Lincoln PowerMig 200

    Forney O/A Rig




  4. #2079
    Join Date
    Mar 2006
    Location
    Yuma, Arizona
    Posts
    3,349

    Re: Welding Fail! post pics here.

    Jess,
    You should look at my post of the fence on the UPRR. That was a mess.
    Lincoln Power Mig 350MP - MIG and Push-Pull
    Lincoln Precision TIG 275,Undercart cooler,Foot/Finger Amptrollers
    Lincoln Hobby-Weld 110v
    Lincoln SP-200 MIG and Hi-Freq Tig
    CK TIG TORCH, gas diffuser, pyrex cup
    Thermal Dynamics Cutmaster 101

  5. #2080
    Join Date
    Apr 2010
    Posts
    2,135

    Re: Welding Fail! post pics here.


    Fnord5


    Quote Originally Posted by Fnord5 View Post
    Opus, once again being a douche. Still waiting on a picture of one of your welds.
    “We are all in the gutter, but some of us are looking at the stars.” Oscar Wilde.

    Be patient - Super Novas are infrequent . . .

    Quote Originally Posted by motolife313 View Post
    Ya maybe you should start a thread that has to do with metal or is your ego to gigantic?
    . . . or is your ego to/too gigantic?

    Quote Originally Posted by Joker11 View Post
    Why has he not been banned yet? Agreed, douche.
    . . . banned yet? = double determiner . . .

    Agreed - is a pluralistic understanding - I question whether your group could plan
    a [welding] crap . . .


    A mere 'douche': is egotistically way-above my security level; from, now forward,
    I wish to be addressed as a Sub-Douche . . .

    I'm - a 'Sensitive New Age Welder' - and respect being put in my place . . .


    Opus



    ps -

    To redirect: Welding Fail! post pics here - is the thread - not panties in a wadd . . .






    .
    Last edited by OPUS FERRO; 07-13-2018 at 12:18 AM. Reason: John C. H. is dead . . .

  6. #2081
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    6,315

    Re: Welding Fail! post pics here.

    Opus how long does it take you to come up with your bs posts?1 hour?

  7. #2082
    Join Date
    Mar 2011
    Location
    Bilbao, Spain
    Posts
    694

    Re: Welding Fail! post pics here.

    I must say that while I don't always concurr with Opus point of view and sometimes he is somewhat blunt, his posts are rather interesting. IMHO!

    Moto, I think everyone (or almost everyone) who has ever worked as an employee, has slacked sometimes at work. But try not to make it too evident!

    Keep the pictures coming!

  8. #2083
    Join Date
    Jan 2016
    Posts
    2,791

    Re: Welding Fail! post pics here.

    Quote Originally Posted by OPUS FERRO View Post

    Fnord5




    “We are all in the gutter, but some of us are looking at the stars.” Oscar Wilde.

    Be patient - Super Novas are infrequent . . .



    . . . or is your ego to/too gigantic?



    . . . banned yet? = double determiner . . .

    Agreed - is a pluralistic understanding - I question whether your group could plan
    a [welding] crap . . .


    A mere 'douche': is egotistically way-above my security level; from, now forward,
    I wish to be addressed as a Sub-Douche . . .

    I'm - a 'Sensitive New Age Welder' - and respect being put in my place . . .


    Opus



    ps -

    To redirect: Welding Fail! post pics here - is the thread - not panties in a wadd . . .






    .
    LOL..be careful what you wish for......

  9. #2084
    Join Date
    Dec 2009
    Location
    Stevens Point, WI
    Posts
    4,299

    Re: Welding Fail! post pics here.

    12v battery, jumper cables, and a 6013.
    I only have a facebook page. https://www.facebook.com/pages/VPT/244788508917829

  10. #2085
    Join Date
    Jul 2011
    Location
    Western Washington
    Posts
    3,580

    Re: Welding Fail! post pics here.

    VPT - what is that on?
    There are no problems. There are only solutions. It's your duty to determine the right one.

    Hobart Handler 210
    Airco 225 Amp MSM Stinger

  11. #2086
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,098

    Re: Welding Fail! post pics here.

    Mower of a design/ predictable failure. This is Ariens mower 5 years old, in pristine condition. No sign of impact. The second photo is the sheet metal deck meant to add stability to the axle assembly.
    Attached Images Attached Images   

  12. #2087
    Join Date
    Dec 2009
    Location
    Stevens Point, WI
    Posts
    4,299

    Re: Welding Fail! post pics here.

    Quote Originally Posted by ThorsHammer View Post
    VPT - what is that on?
    That was the cross member in my Comet.
    12v battery, jumper cables, and a 6013.
    I only have a facebook page. https://www.facebook.com/pages/VPT/244788508917829

  13. #2088
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,098

    Re: Welding Fail! post pics here.

    Thought this was comical. Nice bolts. Must to be difficult to weld vertical in a CAD drawing.
    Attached Images Attached Images  

  14. #2089
    Join Date
    Jun 2008
    Location
    Hardwood Lands, Nova Scotia, Canada
    Posts
    1,721

    Re: Welding Fail! post pics here.

    Never seen that kind of a setup before. Looks like it's concrete sleeve anchors, hope it doesn't have to hold too much, may be ok in shear tho....maybe LOL..............Mike

  15. #2090
    Join Date
    Jul 2014
    Location
    Near San Jose
    Posts
    720

    Re: Welding Fail! post pics here.

    Quote Originally Posted by mrmikey View Post
    Never seen that kind of a setup before. Looks like it's concrete sleeve anchors, hope it doesn't have to hold too much, may be ok in shear tho....maybe LOL..............Mike
    I've seen bolts like that used as expanding anchors for plastic. It uses a simple sleave with slits that make it "flower" as the nut is tightened. The effect is the same as if a washer was installed inside.

    Dan
    ----------------------------
    Measure twice. Weld once. Grind to size.

    MIG: Lincoln SP100
    TIG/STICK: AHP Alphatig 200X

  16. #2091
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    1,103

    Re: Welding Fail! post pics here.

    I have been thinking about buying a shed or metal carport/garage to get some of my lawn stuff out of my shop.
    The local dealer for Leonard truck accessories and buildings had this on their lot. It is their 12x20 metal shed for about $4,300. The studs are 1"x1" and it looks like they were brazed.


    Sent from my SM-G930V using Tapatalk
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 375 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  17. #2092
    Join Date
    Feb 2015
    Posts
    53

    Re: Welding Fail! post pics here.

    So, psacustom, have you made the down-payment yet? I'm ashamed for that to be a product if this country.

  18. #2093
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    1,103

    Re: Welding Fail! post pics here.

    Quote Originally Posted by villageblacksmith View Post
    So, psacustom, have you made the down-payment yet? I'm ashamed for that to be a product if this country.
    Yeah, I think I will hold off buying one of those sheds. I know I could build one much better than that.
    The cheap metal carports at least seem to be better than that.

    Sent from my SM-G930V using Tapatalk
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 375 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  19. #2094
    Join Date
    Apr 2010
    Location
    The Peoples Republic of Kalifornia
    Posts
    3,260

    Re: Welding Fail! post pics here.

    Quote Originally Posted by psacustomcreations View Post
    I have been thinking about buying a shed or metal carport/garage to get some of my lawn stuff out of my shop.
    The local dealer for Leonard truck accessories and buildings had this on their lot. It is their 12x20 metal shed for about $4,300. The studs are 1"x1" and it looks like they were brazed.


    Sent from my SM-G930V using Tapatalk
    Now that is Just Fugly

    Name:  27067360_10155305576886239_5105585799108573142_n.jpg
Views: 853
Size:  51.9 KB


    Name:  uploadfromtaptalk1408854886089.jpg
Views: 849
Size:  47.3 KB
    Backed my CATMA over your CARMA oops clusmy me

    What would SATAN do ??


    Miller Trailblazer 302 AirPak
    Miller Digital Elite
    Optrel Welding Hat
    Arcair K4000
    Suitcase 12RC / 12 VS
    Hypertherm PM-45
    Rage 3 saw
    Rusty old Truck

  20. #2095
    Join Date
    Mar 2006
    Location
    Yuma, Arizona
    Posts
    3,349

    Re: Welding Fail! post pics here.

    Have you found your exhaust manifold bolts keep coming loose?
    Well now you can stop that with some welding and bailing wire!


    Name:  038216FD-3869-4544-B10A-551134E06601.jpeg
Views: 737
Size:  105.8 KB
    Lincoln Power Mig 350MP - MIG and Push-Pull
    Lincoln Precision TIG 275,Undercart cooler,Foot/Finger Amptrollers
    Lincoln Hobby-Weld 110v
    Lincoln SP-200 MIG and Hi-Freq Tig
    CK TIG TORCH, gas diffuser, pyrex cup
    Thermal Dynamics Cutmaster 101

  21. #2096
    Join Date
    Dec 2013
    Location
    Pa
    Posts
    893

    Re: Welding Fail! post pics here.

    I bet psacreations shed if he buys it those(bird poop/splatter) will no fail. It's amazing how shiiiity stuff will stand.

  22. #2097
    Join Date
    Jul 2011
    Location
    Western Washington
    Posts
    3,580

    Re: Welding Fail! post pics here.

    Quote Originally Posted by Joker11 View Post
    Have you found your exhaust manifold bolts keep coming loose?
    Well now you can stop that with some welding and bailing wire!


    Name:  038216FD-3869-4544-B10A-551134E06601.jpeg
Views: 737
Size:  105.8 KB
    while I applaud their problem solving skills, that's just hilarious.
    There are no problems. There are only solutions. It's your duty to determine the right one.

    Hobart Handler 210
    Airco 225 Amp MSM Stinger

  23. #2098
    Join Date
    Mar 2014
    Posts
    145

    Re: Welding Fail! post pics here.

    Just another form of loctite.... the non-liquid type.

  24. #2099
    Join Date
    Dec 2015
    Location
    Southeast,Florida
    Posts
    89

    Re: Welding Fail! post pics here.

    Quote Originally Posted by Joker11 View Post
    Have you found your exhaust manifold bolts keep coming loose?
    Well now you can stop that with some welding and bailing wire!


    Name:  038216FD-3869-4544-B10A-551134E06601.jpeg
Views: 737
Size:  105.8 KB
    There is a better way
    Name:  spinner5-w.jpg
Views: 1104
Size:  39.7 KB
    Imagination is more important than knowledge. - Albert Einstein

    I wanted a mission and for my sins, they gave me one. - Captain Benjamin L. Willard

  25. #2100
    Join Date
    May 2018
    Location
    Land of the Toxic Avenger
    Posts
    542

    Re: Welding Fail! post pics here.

    This guy needs a good welder. The yellow ratcheting strap is better suited elsewhere
    Attached Images Attached Images  
    T man.


    15 + years working for myself, and by golly, I still don't know what I want to do when I grow up.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  