  1. #76
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,364

    Re: Home made tools!

    Quote Originally Posted by Magnetic Mechanic View Post
    make sure the end of the ball is centered in the tee
    Neat little home-made eductor MM. We use slightly more refined devices for fire fighting foam proportioning.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  2. #77
    Join Date
    Jan 2008
    Location
    Arkansas
    Posts
    1,202

    Re: Home made tools!

    Thats where i got the idea from - fire fighting school, USN Philadelphia 1965.
    A butterfly without wings,
    is just an ugly bug


  3. #78
    Join Date
    Dec 2008
    Location
    La Vernia, Tx
    Posts
    59

    Re: Home made tools!

    Quote Originally Posted by littlefuzz View Post
    Here's the press I made a couple of weeks ago and I made a set of the roller stands that are to the right in the pic.
    Attachment 25191
    It is better than one bought at a store.

  4. #79

  5. #80
    Join Date
    Feb 2008
    Location
    Massachusetts
    Posts
    100

    Re: Home made tools!


    6ton barrel vise / press......A few pieces of angle iron, a couple of 3/4" bolts and a cheap hydraulic jack.....BINGO!




    Action Puller.......Used to "pop" a rifle action out of the stock after epoxy bedding


    Various "Barrel Blocks" to use with barrel vise above.....


    Reloading trays to hold cartridges while reloading. Made from Air Conditioner suspended ceiling grills.
    Roy B
    Dartmouth, Ma

    http://www.rvbprecision.com

    MM 185 MIG
    Diversion 165
    Purox W200 O/A
    Grizzly 9957 Mill
    Grizzly 4030 Metal Band Saw
    Grizzly 1050 Knife Belt Sander
    Jet 1236 Metal Lathe
    CM 14" Metal Band Saw
    TP Blast Cabinet

  6. #81
    Join Date
    Oct 2007
    Posts
    152

    Re: Home made tools!

    Got tired of forking over ridiculous bucks for moto tire changes.
    Works good on car tires too.

    Last edited by sunline; 12-11-2008 at 11:32 AM.
    Airco 300 squarewave
    Mig welding center...
    Powcon sm300/LN 25
    Powcon sm200/PD l
    Hypertherm PM 1100
    Miller AEAD 200LE W/LN25 FC
    and now another sm200 pd l combo.

  7. #82
    Join Date
    Dec 2008
    Location
    Long Island, New York
    Posts
    133

    Re: Home made tools!

    tube roller with dies cut on a wood lathe out of Delrin (have held up so far)




    my first bender - uses pro-tools dies



    new hydro bender - uses pro-tools dies


  8. #83
    Join Date
    Aug 2007
    Location
    Netherlands
    Posts
    177

    Re: Home made tools!

    Great stuff.

  9. #84
    Join Date
    Dec 2008
    Posts
    235

    Re: Home made tools!

    came across this thread tonight, man I am excited. I will be copying a lot of your guys stuff, this stuff is great, ideas, ingenuity, and improvising. I LOVE IT here's a few that I had laying around, they don't really compare, they are all realitivaly cheap and readily available, but when you don't have the patience to run to the tool store or wait for the snap on guy this what I have made... more to come
    Attached Images Attached Images    

  10. #85
    Join Date
    Jul 2007
    Location
    Denmark, Zealand
    Posts
    122

    Re: Home made tools!

    I just made this today, and its one heavy duty scratching thingy, for drawing lines on steel, i don't know the translation

    http://www.box.net/shared/i9e0hx4yin

    http://www.box.net/shared/qy3ij7i10n
    ¤
    If you got money, i've got time

  11. #86
    Join Date
    Jan 2008
    Location
    Arkansas
    Posts
    1,202

    Re: Home made tools!

    A "SCRIBE" perhaps
    A butterfly without wings,
    is just an ugly bug


  12. #87
    Join Date
    Jul 2007
    Location
    Denmark, Zealand
    Posts
    122

    Re: Home made tools!

    That must be it,

    Because if the translate the danish word directly to english it becomes "Scratching Spike"
    ¤
    If you got money, i've got time

  13. #88
    Join Date
    Nov 2008
    Location
    Texas Near Dallas
    Posts
    1,075

    Re: Home made tools!


    Tool for standing up 2"x6" tubing used for lath. Works wonders when the entire length is a few hundred pounds and you're sitting on a 4" I-beam flange. 4" isn't really enough for a whole buttcheek.

    Dynasty200DX w/coolmate1
    MM210
    MM Vintage
    ESAB miniarc161lts
    Lincoln AC225
    Victor O/A, Smith AW1A
    Cutmaster 81
    IR 2475N7.5FP
    Rage3
    Jancy USA101
    9" SB
    AEAD-200LE

  14. #89
    Join Date
    Nov 2008
    Location
    Huntington, In
    Posts
    1,267

    Re: Home made tools!

    OK!
    Here's my contribution.
    One of the tools I have made, its a bending jig, made for bending flat stock of up to 4" wide, I have used this to bend up to 1/2" thick stock, and can bend as short as 2" from one bend to another!
    I made the jig for a smaller shop press that I had, and am now converting it to be used on this monster! "The second pic"
    Attached Images Attached Images   
    #1. If you don't like what I wrote, or if it offends you, then don't read it!
    #2. I am living life the way I see fit, if you don't like the way I'M living, tough sh**!

  15. #90
    Join Date
    Nov 2008
    Location
    Huntington, In
    Posts
    1,267

    Re: Home made tools!

    This is one of the bigger tools I have made!
    I am now making one even bigger.
    Attached Images Attached Images  
    #1. If you don't like what I wrote, or if it offends you, then don't read it!
    #2. I am living life the way I see fit, if you don't like the way I'M living, tough sh**!

  16. #91
    Join Date
    Nov 2008
    Location
    Texas Near Dallas
    Posts
    1,075

    Re: Home made tools!

    Here's a "poor man's" faceplate I made for a friends wood lathe.


    I welded a nut with the threads that match his lathe spindle to a chunk of 3/4" plate. Then mounted it on a piece of all-thread, chuck it in the metal lathe, turned the plate into a circle and faced it off. I've just recently started using a metal lathe and my skills are not so good. I couldn't get a very nice finish. The facing was fair, but the outside edge kept chattering. I don't think I'm grinding my tool bits correctly (HSS). It'll be good enough for wood working.

    Dynasty200DX w/coolmate1
    MM210
    MM Vintage
    ESAB miniarc161lts
    Lincoln AC225
    Victor O/A, Smith AW1A
    Cutmaster 81
    IR 2475N7.5FP
    Rage3
    Jancy USA101
    9" SB
    AEAD-200LE

  17. #92
    Join Date
    Aug 2007
    Location
    Netherlands
    Posts
    177

    Re: Home made tools!

    Make sure that:
    The chissel is right on centre
    The angles are right
    There's not too much freeplay in the cross slide

    Then you should be ok.

  18. #93
    Join Date
    Sep 2006
    Location
    Marlborough, The Peoples Republik of MA
    Posts
    3,559

    Re: Home made tools!

    Just some handy dandy dogs, they do the trick everytime.


    Disclaimer; "I am just an a$$hole welder, don't take it personally ."

  19. #94
    Join Date
    Jan 2008
    Posts
    3,456

    Re: Home made tools!

    dogs handy dandy deedy dey do..very cool mon

  20. #95
    Join Date
    Sep 2008
    Location
    Central PA
    Posts
    1,964

    Re: Home made tools!

    Toz, I like them dogs.

  21. #96
    Join Date
    Dec 2007
    Location
    Western PA
    Posts
    1,258

    Re: Home made tools!

    Woof!

  22. #97
    Join Date
    Dec 2006
    Posts
    54

    Re: Home made tools!

    nice job everyone....my problem is not enough time and too many ideas in my head

    anyone ever made a rotisserie for welding pipes with a 3 or 4 jaw lathe chuck and variable speed motor ?
    My weekend hobby -


  23. #98
    Join Date
    Mar 2009
    Location
    upland, ca
    Posts
    1,102

    Re: Home made tools!

    this thread should be stickied

  24. #99
    Join Date
    Jan 2008
    Location
    Arkansas
    Posts
    1,202

    Re: Home made tools!

    "this thread should be stickied"

    Define stickied please.
    A butterfly without wings,
    is just an ugly bug


  25. #100
    Join Date
    Jun 2008
    Location
    Central California
    Posts
    3,745

    Re: Home made tools!

    Posted by AndyA:
    I welded a nut with the threads that match his lathe spindle to a chunk of 3/4" plate. Then mounted it on a piece of all-thread, chuck it in the metal lathe, turned the plate into a circle and faced it off. I've just recently started using a metal lathe and my skills are not so good. I couldn't get a very nice finish. The facing was fair, but the outside edge kept chattering. I don't think I'm grinding my tool bits correctly (HSS). It'll be good enough for wood working.
    I would have thought you could get a better hold on it by chucking the nut in a three-jaw, and using a live center on the back side if needed. Also, taking a light, fine cut with a nearly squared edge rather than using a more rounded tool will cut the chatter for the last cut.

    You might find that the libraries in your area have some basic machining textbooks. If not, (ours threw stuff like that away long ago; isn't PC), take a look at the reprints of old manuals and such at

    Lindsay Publications

    Lots of interesting and reasonably priced material here. Even some stuff on a new field they call 'Welding'!

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement