Compressor explosions - Page 4
RSS | Subscribe | Contact Us | Advertise | About Us
Page 4 of 4 FirstFirst ... 234
Results 76 to 87 of 87
  1. #76
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,064

    Re: Compressor explosions

    Quote Originally Posted by blackbart View Post
    I actually answered that craigs list ad with a link to this thread.
    Lol. I doubt that they will have their mind changed.

  2. #77
    Join Date
    Jun 2010
    Posts
    1,865

    Re: Compressor explosions

    I have welded many tanks myself too. Now I'm rethinking those!

  3. #78
    Join Date
    Jun 2010
    Posts
    1,865

    Re: Compressor explosions

    ForHire, I did the 2 liter soda bottle experiment with a bunch of kids for a science fair. We were making them into rockets, building a release trigger into the design. They would go up 100' with the right ratio of air and water. They are also powerful, they would work even with a basketball on them.
    The same kids wanted to separate oxygen and hydrogen. I put a couple ounces in a bottle with the rest being water. I lit it off and everyone got soaked. After that the kids stopped making a separator that filled 33 gal trash cans. They wanted to make a hydrogen powered car. I think I convinced them they would level the neighborhood.

  4. #79
    Join Date
    Oct 2010
    Location
    S.E. Michigan
    Posts
    397

    Re: Compressor explosions

    Quote Originally Posted by Joker11 View Post
    sidecarflip,
    Sorry. I actually did read that first. I just forgot I read it. My bad.
    No problem. I just happen to work for a major supplier of Hot Rolled Sheet Products and Hot dip and electro galvanized sheet. We sell a ,lot of 100X AKDQ deep draw high strength sheet to companies that draw and form compressor tanks and propane CNG tanks. Chem-Trol being one.

    I'm just in the trucking end. They own a very large private fleet to deliver their products, but I get to fiddle around in the plants when I want to.

    I'm a safety officer, aka, that SOB with the camera.

  5. #80
    Join Date
    Jun 2010
    Posts
    1,865

    Re: Compressor explosions

    I just realized the concrete trucks around here use there air to pressurize a water tank much like my design, any thoughts on it? I could actually make my design with no welding, just a saddle type mount instead.

  6. #81
    Join Date
    Jul 2008
    Location
    Long Island
    Posts
    3,003

    Re: Compressor explosions

    Re-read this thread. That was covered above here. People have died when water tanks on concrete trucks exploded.

  7. #82
    Join Date
    Sep 2006
    Location
    NJ, USA
    Posts
    3,431

    Re: Compressor explosions

    Quote Originally Posted by blackbart View Post
    I just realized the concrete trucks around here use there air to pressurize a water tank much like my design, any thoughts on it? I could actually make my design with no welding, just a saddle type mount instead.
    Idiot OEM made an aluminum pressure vessel without following the pressure vessel Codes and tried to claim it wasn't a pressure vessel after several injuries and fatalities due to said 'pressure-vessel-that-isn't-a-pressure-vessel' failed catastrophically.

    ASME pointedly said 'You made a pressure vessel'.

    OEM lost the lawsuits.

    If you want to make a pressure vessel, follow all of the applicable Codes.

    Otherwise, make a water tank and put a pump and hose on it.

    IMNSHO.
    The best laid schemes ... Gang oft agley ...

  8. #83
    Join Date
    Jun 2010
    Posts
    1,865

    Re: Compressor explosions

    Pretty bad when I didn't catch that on my own thread. I wish there was an easy answer, these things put out a lot of fires! It looks like I'm going back to a pump design! There are companies that make ones like mine 3000 gallons! They charge with vacuum to fill with no pump and discgarge with air pressure. Basically they look like a propane truck. I'm sure they have a lot more permits and certs than I do!

  9. #84
    Join Date
    Jun 2012
    Location
    Bemidji MN
    Posts
    14,109

    Re: Compressor explosions

    Quote Originally Posted by rlitman View Post
    Re-read this thread. That was covered above here. People have died when water tanks on concrete trucks exploded.
    I used to drive concrete trucks where we pressured the water tanks.....

    and they were old and crappy looking.....crap

    Dave J.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  10. #85
    Join Date
    Jun 2010
    Posts
    1,865

    Re: Compressor explosions

    The ones here in Ca still use them, that's why I wondered who certifies them.

  11. #86
    Join Date
    Sep 2006
    Location
    NJ, USA
    Posts
    3,431

    Re: Compressor explosions

    Quote Originally Posted by blackbart View Post
    The ones here in Ca still use them, that's why I wondered who certifies them.
    Send Cal-OSHA after them.
    The best laid schemes ... Gang oft agley ...

  12. #87
    Join Date
    Jun 2010
    Posts
    1,865

    Re: Compressor explosions

    That......I wouldn't do to my worst enemies!

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement