    This thread is about making MIG look TIG, or really nice looking mig welds.

    I am going to try something.

    ONLY POST IF YOU HAVE A PICTURE OF YOUR OWN WORK.

    The point is we want to SEE your attempt.

    I am going to try to master this too.

    Here is my picture. It aint like ZTfabs, but it was about 200 feet of weld.


    WFS 330 of .035, about 20 volts C/25. This is 3/16" square tubing so there is a natural perfect fit up. I should have been at around 200 amps.

    Name:  2beads.jpg
Views: 58059
Size:  73.3 KB

    Horizontal, making circles going up on the forward stroke. First pass on clean bare steal, second pass down through the puddle. I turn the heat WAY UP to do this. 200 amps on 3/16" horizontal groove.
    Here is a link to another thread

    http://weldingweb.com/showthread.php...hlight=mig+tig




    Nothing discussed here but Mig welds.



    David

    edit: Mig gun was held straight in the joint.
    Last edited by David R; 05-26-2009 at 05:56 PM.
    Real world weldin.

    When I grow up I want to be a tig weldor.

  2. #2
    Join Date
    May 2009
    Location
    texas
    Posts
    2

    Re: Mig like Tig

    i have never tried to tig weld i was wanting to know if it is at all harder than stick, i need to know cause works gettin scarace and i may have to go singel hand and they say combo pays better

  3. #3
    Join Date
    Jan 2008
    Posts
    3,456

    Re: Mig like Tig

    harder shmarder, its different. its like oa welding, heat in one hand to make the puddle, and filler in the other to feed it. in ways its easier than stick , cause thers no slag to block yer view, you see the molten metal and its up to you to make sure it goes where it should.

  4. #4
    Join Date
    Feb 2007
    Location
    Hamlin NY
    Posts
    7,303

    My attempt

    I was welding bucket teeth on using a forward whip and bare wire.



    Name:  bucket.jpg
Views: 57708
Size:  39.1 KB


    Mig welds that look like tig welds or attempts at it.

    David
    Real world weldin.

    When I grow up I want to be a tig weldor.

  5. #5
    Join Date
    Apr 2009
    Location
    Virginia USA
    Posts
    95

    Re: My attempt

    Just curious, is this a new fashion thing or is their some good technical reason to make MIG look like TIG??

  6. #6
    Join Date
    Feb 2007
    Location
    Hamlin NY
    Posts
    7,303

    Re: Mig like Tig

    Take a look here and see what started this.

    http://weldingweb.com/showthread.php?t=30507

    Along with other threads about the same thing.

    This is a trial thread.

    David
    Real world weldin.

    When I grow up I want to be a tig weldor.

  7. #7
    Join Date
    Jul 2006
    Location
    Royse City, Texas (Dallas area)
    Posts
    859

    Re: Mig like Tig

    Here is an image that I got out of my welders manual. It shows that dragging is a real method which was challenged in another thread.

    Also a meager attempt of getting the tig weld look on some crappy rusty steel. There is a photo of the welds and a photo of the inside of the box.

    I did not have good steel to try it on but will try to get something better soon.

    Bob
    Attached Images Attached Images    



  8. #8
    Join Date
    Apr 2009
    Location
    Colorado
    Posts
    18

    Re: Mig like Tig

    I'm glad you started this thread David. I've been wanting to try doing this and just needed a reason.

    Lincoln 100 HD with .030" NR-211-MP on some 1 1/4" X 1/8" angle iron. I didn't hold it at the end quite long enough but it ain't too bad after about 5 minutes of playing around. The dime is partially covering a tack, I ran a few beads on the other side before trying this one.

    I may re-post this one so you guys can critique it without hijacking this thread.


  9. #9
    Join Date
    Nov 2007
    Location
    Pittsburgh Pennsylvania
    Posts
    1,330

    Re: Mig like Tig

    Here was my attempt on 3/8 plate to 5/8 roundbar. I used a lincoln weld pak and .035 lincoln innershield nr211mp wire. This was a table mount for my sander.
    Shane
    Attached Images Attached Images    
    Ya gotta spend money to make money!

  10. #10
    Join Date
    Feb 2007
    Posts
    557

    Re: My attempt

    Quote Originally Posted by GerryR View Post
    Just curious, is this a new fashion thing or is their some good technical reason to make MIG look like TIG??
    For my business - custom off road fabrication- it is the customers perception that these types of welds are better. Of course, appearance doesn't really have much to do with the quality. As welders we know that, but for me, aesthetically appealing welds help sales.


    Here is a pic of a Dana 60 axle housing I mig welded to the tubes.
    Attached Images Attached Images  

  11. #11
    Join Date
    Aug 2006
    Location
    San Dimas, CA
    Posts
    3,033

    Re: Mig like Tig

    Here's a couple of my attempts at it.

    These were some prototype brackets, .125" CRS.





    This is a truss that I made for a 9" differential housing: I cut the truss from 2"x3"x.125" tubing.





    And here is the "box" from the previous thread. It is actually a cover for an old rooftop hatch that was de-commissioned. .125" CRS.







    http://all-a-cart.com

    Welding Cart Kits and accessories

  12. #12
    Join Date
    Feb 2007
    Posts
    557

    Re: Mig like Tig

    Quote Originally Posted by ZTFab View Post
    Here's a couple of my attempts at it.

    "attempts" - that's funny right there!

  13. #13
    Join Date
    Aug 2006
    Location
    San Dimas, CA
    Posts
    3,033

    Re: Mig like Tig

    Here's a few more...

    .125" and .188" CRS.

    These are both open corner joints like the "box". THere is a small piece with a lap joint on the .188" as well.









    http://all-a-cart.com

    Welding Cart Kits and accessories

  14. #14
    Join Date
    Dec 2008
    Location
    N.E. oHIo
    Posts
    365

    Re: Mig like Tig----I'm ready for a critique!

    My first attempts were more like "MIG like MIG".
    I cut 8 coupons of 1/8" CRS and tacked them to give myself open groove joints.
    This was also my first try at pulling the torch, I usually push.

    Each coupon was welded in 2 steps, from the corner to the center tack, left to right, with changes in WFS and voltage made on each half. You can see the reference marks: 1A/1B,
    2A/2B, etc.

    Basic settings:
    Lincoln PM300 in GMAW (#5) mode....no pulse.
    .035" ER70-6
    92/8 Ar/Co2

    Coupons tacked but needing cleaned. The "Spot" feature is cool! .5sec duration.


    Coupon 1: A side, 150 WFS / 20 volts Too Hot!!....B side, 150 WFS / 17.5 volts.



    Coupon 2: A side, 140 WFS / 17.5 volts....B side, 140 WFS / 16 volts....still hot.



    Coupon 3: A side, 130 WFS / 16 volts....B side, 130 WFS / 15 volts....unstable arc @ 15volts, 16 seems mo' better.



    Coupon 4: A side, 120 WFS / 16 volts....B side, 110 WFS / 16 volts.



    Coupon 4A seems to be the best of the lot, from a WFS/Volts standpoint. I think my technique of making the "e" is too slow. Like, I'm not taking the horizontal move far enough to the right before I curve back around counter clockwise.

    I spent about 1/2 an hour doing "dry runs" with the machine turned off so as to get a feel for the drag/"e" technique. The 400 amp gun is definitely NOT the one for this!

    Comments and pointers will be appreciated!


    Rex

  15. #15
    Join Date
    Mar 2009
    Location
    Mississippi
    Posts
    714

    Re: Mig like Tig

    No fair! I think Paul should be excluded from this "attempt"

    Michael Jordan: "Just put this ball through that loop? Sure, I'll try it"

  16. #16
    Join Date
    Feb 2007
    Location
    Hamlin NY
    Posts
    7,303

    Re: Mig like Tig

    Amps or heat is the wire speed.

    Volts are the bead width. You can see that in your cupons.

    I would try 120 to 130 ipm with about 17 -18 volts. To your own taste of course.....

    If you look at cupon 3, A side you are close, but there is too much weld or wire.

    you could also try straight in and push.

    I like the attempts, looks like you are on your way!

    More please

    David
    Last edited by David R; 05-27-2009 at 07:20 PM.
    Real world weldin.

    When I grow up I want to be a tig weldor.

  17. #17
    Join Date
    Jan 2004
    Posts
    1,571

    Re: Mig like Tig

    Here are a few sample T joints that I ran quite a while ago.
    Attached Images Attached Images    

  18. #18

    Re: Mig like Tig


  19. #19
    Join Date
    Nov 2008
    Location
    Florida
    Posts
    29

    Re: Mig like Tig



    It is a small part, but that is all I have in here right now. I honestly can't remember if I pushed or pulled this one. I push/pull based on which side I am coming from and what I can do to get comfortable. I can also weld with either hand so right to left or left to right doesn't bother me.

    For a comparison, here is a small tig weld I did recently.

    Jamie Webb
    Welder & Inspector
    Business and Hobby
    Lincoln Pro-Mig 180 with Spool Gun and Lincoln AC225

  20. #20
    Join Date
    Aug 2006
    Location
    San Dimas, CA
    Posts
    3,033

    Re: Mig like Tig

    Quote Originally Posted by Dan View Post
    Here are a few sample T joints that I ran quite a while ago.
    Those are beautiful welds Dan.
    http://all-a-cart.com

    Welding Cart Kits and accessories

  21. #21
    Join Date
    Apr 2009
    Location
    St. Pete, FL
    Posts
    44

    Re: Mig like Tig

    I hate guys that weld like that It's beautiful work, you make us all proud...I know you've listed it before, but ZT could you give your parameters again? I've got an itch to give it a go too. Hat's off to all those that showed up on this! Thanks

    maniak

  22. #22
    Join Date
    Feb 2009
    Location
    mountain west
    Posts
    128

    Re: Mig like Tig

    That axle truss is art.

    Just realised, referencing another thread, GOOD ART. didn't want any mistakes here.
    past work toys; lathes,mills, drills, saws, robots, lasers ironworker, shears, brake, press, grinders, tensile tester, torches, tigs, migs, sticks, platten table, positioner, plasmas , gleeble and spot. Retired June 30, 2009.

  23. #23
    Join Date
    Aug 2006
    Location
    San Dimas, CA
    Posts
    3,033

    Re: Mig like Tig

    Quote Originally Posted by wesdavidson View Post
    That axle truss is art.

    Just realised, referencing another thread, GOOD ART. didn't want any mistakes here.
    Thanks.

    I like this one that I did a little better. It's in two separate threads.

    http://weldingweb.com/showthread.php?t=10922

    http://weldingweb.com/showthread.php?t=11016
    http://all-a-cart.com

    Welding Cart Kits and accessories

  24. #24
    Join Date
    Aug 2006
    Location
    San Dimas, CA
    Posts
    3,033

    Re: Mig like Tig

    Quote Originally Posted by maniak View Post
    I hate guys that weld like that It's beautiful work, you make us all proud...I know you've listed it before, but ZT could you give your parameters again? I've got an itch to give it a go too. Hat's off to all those that showed up on this! Thanks

    maniak
    Any weld in particular? I posted a couple of different ones and they would obviously have different settings.
    http://all-a-cart.com

    Welding Cart Kits and accessories

  25. #25
    Join Date
    May 2007
    Location
    SoCal
    Posts
    4,785

    Re: Mig like Tig

    I wouldn't want my mig welds to look like tig. Clean and consistant, yes! But not like tig, it ain't natural. The best from my days leading up to certifying.

    Lincoln V350 Pro @ 18.~plus volts and LN-7 wire feeder @ 225-ish? ipm.
    Here are some tig beads from cyberspace...yeah, I can do that!
    Attached Images Attached Images  
    City of L.A. Structural; Manual & Semi-Automatic;
    "Surely there is a mine for silver, and a place where gold is refined. Iron is taken from the earth, and copper is smelted from ore."
    Job 28:1,2

    Lincoln, Miller, Victor & ISV Bible

    Danny

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement