  1. #451
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    621

    Re: Blacksmithing tools

    Just in case idacal gets frustrated with his project, I’d be more than happy to take it off his hands.
    ​Terry

    **FORNEY**
    180
    230
    **THERMAL ARC**
    210 Fabricator
    181i
    **LINCOLN**
    Idealarc 250/250
    SA 200 (2)
    Ranger 305G LN-25 Pro
    **MILLER**
    Spectrum 625
    Maxstar 150STL
    Syncrowave 351
    XMT 350 cc/cv
    MM 350P

  2. #452
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    1,842

    Re: Blacksmithing tools

    I got lost in southern England many moons ago... ended up driving out onto a beach and was parked on a large concrete slab looking for the road map. About the time I was reaching for the map I looked up and saw the sign, "Danger. Hovercraft Landing Pad." Apparently it was where you caught the Hovercraft to France before the chunnel was finished. I moved very quickly.
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  3. #453
    Join Date
    Aug 2014
    Location
    Cerritos, CA
    Posts
    150

    Re: Blacksmithing tools

    Modified an estwing tack hammer today, for small rivets, advice from Jacob Faram. Also tried a brass rivet eye I've seen Faram do. With his permission of course. First attempt sucked, but I like the accent.



    Sent from my SM-N950U using Tapatalk

  4. #454
    Join Date
    Sep 2013
    Posts
    309

    Re: Blacksmithing tools

    Very nice, Mud.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement