Building A Tig Water Cooler For Dummies!!! - Page 3
RSS | Subscribe | Contact Us | Advertise | About Us
Page 3 of 5 FirstFirst 12345 LastLast
Results 51 to 75 of 101
  1. #51
    Join Date
    Dec 2011
    Posts
    951

    Re: Building A Tig Water Cooler For Dummies!!!

    Quote Originally Posted by AluminumWelder View Post
    Lets say you have the sheet metal to make the liquid tank but have to buy everything else.
    How much time and $$$ is spent making your own?
    there are chineesse tig water coolers on ebay for $375, they are the same ones that everylast and longevity sell.

    Help me determine what savings if any are achieved by DIY?
    I don't know how much I will have in this..........but..........I enjoy building things for myself!

  2. #52
    Join Date
    Aug 2014
    Location
    Long Island
    Posts
    121

    Re: Building A Tig Water Cooler For Dummies!!!

    how about using parts that they use to cool computers and laser ? inexspensive and sized right Name:  radiator.jpg
Views: 3768
Size:  28.6 KB

  3. #53
    Join Date
    Jun 2014
    Location
    Central Nebraska
    Posts
    69

    Re: Building A Tig Water Cooler For Dummies!!!

    I stole this from another thread that google led me to. This was a VERY clean build using computer cooling components like mentioned above.

    Scroll down to posts 26-30

    http://www.advrider.com/forums/showt...=640590&page=2

  4. #54
    Join Date
    Dec 2014
    Location
    surrey bc
    Posts
    4

    Re: Building A Tig Water Cooler For Dummies!!!

    I used an aquarium pump and 50 gallon drum in a machine shop I worked at running 300 amps on copper induction coils for case hardening for hours at a time. I bet you could use a smaller beer keg since the drum was only ever half full anyways. The water never required a chiller since the volume was so large and it just ran on windshield washer hose lines same as my argon lines. The tool and die makers had it setup when I started and I used a 90 or 110 cfm bathroom fan with alum flexible dryer tubing for fume extraction to the outside.

  5. #55
    Join Date
    Dec 2013
    Posts
    454

    Re: Building A Tig Water Cooler For Dummies!!!

    Not that inexpensive actually but easier to configure than a car heater core (1959 Olds 88 comes to mind as the largest one I could find, which was $71 at Rock auto). Then you have to wonder is it aluminum or copper etc. At least the PC rads tell you up front whether it is copper with brass tanks or aluminum etc.

    Anyway you don't really need a radiator or a fan unless you are maxed out on 200A or more all the time on a high duty cycle in high ambient temps.

    The small annular gear pump is the genius move if you can find one. You could have a totally silent cooler that way.

  6. #56
    Join Date
    May 2006
    Location
    Northern California
    Posts
    1,840

    Re: Building A Tig Water Cooler For Dummies!!!

    You can add a radiator if you want but they really aren't necessary. I have two coolers. One is a Barnard with a radiator and the other is a home built with a large tank. Neither one of them has ever gotten hot but I seldom weld at high amperages. I use Procon pumps in both coolers. They are excellent.
    Miller Millermatic 252
    Miller Syncrowave 200
    Liincoln AC-DC 225
    Victor O-A Set

  7. #57
    Join Date
    Dec 2011
    Posts
    951

    Re: Building A Tig Water Cooler For Dummies!!!

    Finally acquired a Procon pump and a motor. Got it put together tonight.......tried it with my TA 185 maxed out and all was cool. I made it portable so it use it on different machines.

    Like to thank all who help on this project.







    Last edited by rahtreelimbs; 01-26-2015 at 11:03 PM.

  8. #58
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    8,443

    Re: Building A Tig Water Cooler For Dummies!!!

    Great job! Glad it works good for you. I need one bad for my pt225

  9. #59
    Join Date
    Mar 2014
    Location
    North East Indiana
    Posts
    447

    Re: Building A Tig Water Cooler For Dummies!!!

    Quote Originally Posted by rahtreelimbs View Post
    Finally acquired a Procon pump and a motor. Got it put together tonight.......tried it with my TA 185 maxed out and all was cool. I made it portable so it use it on different machines.

    Like to thank all who help on this project.







    Where did you pick up those quick disconnects?

  10. #60
    Join Date
    Feb 2009
    Location
    Chicago
    Posts
    6,211

    Re: Building A Tig Water Cooler For Dummies!!!

    Great now I want to build one
    Great work!!
    Torchmate 2x2 CNC with Flashcut CNC controls
    Hypertherm Powermax45
    2015 AHP Tig
    Razorweld 195 Mig
    Razorweld 200ac/dc Tig
    ViperMig 180
    Razorweld, Vipercut/Vipermig, SSC Foot Pedal & MK Products & Atlas Positioner Dealer

  11. #61
    Join Date
    Mar 2014
    Location
    Savannah, Georgia
    Posts
    273

    Re: Building A Tig Water Cooler For Dummies!!!

    Wow, this is very interesting. Makes me want to construct one as well and I don't even need one!
    I really have no idea what I am doing.
    Two Shop Cats (not Bobcats...real cats)
    Miller DialArc 250 AC/DC
    Scratch-Start TIG Setup
    MIG 175
    Plasma Cutter
    O/A

  12. #62
    Join Date
    Dec 2011
    Posts
    951

    Re: Building A Tig Water Cooler For Dummies!!!

    Quote Originally Posted by turismolover22 View Post
    Where did you pick up those quick disconnects?
    USA Weld.

  13. #63
    Join Date
    Oct 2013
    Location
    W. WA
    Posts
    455

    Re: Building A Tig Water Cooler For Dummies!!!

    Nice job!!

    DB

  14. #64
    Join Date
    Dec 2011
    Posts
    951

    Re: Building A Tig Water Cooler For Dummies!!!

    Finally got the cooler all done. I added a cover for nothing other than looks While I was at it I added a second fan. The radiator is close to the motor and I wanted to get enough air flow. The two big holes are for the fans and the small hole is to read the pressure gauge. The cover I bent up out of .060 clear anodized sheet.





    Last edited by rahtreelimbs; 02-11-2015 at 09:52 PM.

  15. #65
    Join Date
    Feb 2009
    Location
    Chicago
    Posts
    6,211

    Re: Building A Tig Water Cooler For Dummies!!!

    Looking good dude! That came out good looking
    Torchmate 2x2 CNC with Flashcut CNC controls
    Hypertherm Powermax45
    2015 AHP Tig
    Razorweld 195 Mig
    Razorweld 200ac/dc Tig
    ViperMig 180
    Razorweld, Vipercut/Vipermig, SSC Foot Pedal & MK Products & Atlas Positioner Dealer

  16. #66
    Join Date
    Dec 2010
    Location
    Utah
    Posts
    2,082

    Re: Building A Tig Water Cooler For Dummies!!!

    Looks good. The way I plumb, I would be worried about leaks and not being able to see them.

  17. #67
    Join Date
    Feb 2011
    Posts
    29

    Re: Building A Tig Water Cooler For Dummies!!!

    How about the quick connect fittings -- Do they seal or must you drain the hoses when disconnected?

    I just got my ebay carbonator today -- I'd love to do quick connect fittings but would hate to have to drain the hose every time I take it apart

  18. #68
    Join Date
    Sep 2014
    Location
    In the 209
    Posts
    1,044

    Re: Building A Tig Water Cooler For Dummies!!!

    Quote Originally Posted by Heavyopp View Post
    How about the quick connect fittings -- Do they seal or must you drain the hoses when disconnected?

    I just got my ebay carbonator today -- I'd love to do quick connect fittings but would hate to have to drain the hose every time I take it apart
    What is this carbonator you speak of?


    Sent from my dumb smartphone
    Teach Ag Mech - Mike

    At Home:
    Lincoln Electric AC225
    Miller Challenger 172
    Gas Axe

    Work:
    eclectic bunch of 90's vintage blue boxes

  19. #69
    Join Date
    Feb 2011
    Posts
    29

    Re: Building A Tig Water Cooler For Dummies!!!

    Quote Originally Posted by teachagmech View Post
    What is this carbonator you speak of?


    Sent from my dumb smartphone
    A carbonator is used to inject co2 into water making seltzer -- I has a 2 gallon stainless tank, motor and a procon pump with misc water lines -- All the main parts you need to make a tig cooler

    for the cool price of $75 shipped to my home -- This is the base for my home built...

  20. #70
    Join Date
    Sep 2014
    Location
    In the 209
    Posts
    1,044

    Re: Building A Tig Water Cooler For Dummies!!!

    Nice!


    Sent from my dumb smartphone
    Teach Ag Mech - Mike

    At Home:
    Lincoln Electric AC225
    Miller Challenger 172
    Gas Axe

    Work:
    eclectic bunch of 90's vintage blue boxes

  21. #71
    Join Date
    Jan 2015
    Location
    Tampa
    Posts
    13

    Re: Building A Tig Water Cooler For Dummies!!!

    I built my own cart using a standard Procon pump, Marathon electric 1/3 HP AC motor, and stainless 1/2" tubing and fittings. The reservoir is a piece of 6" sanitary tubing that holds about 2 gallons. I have a temperature gauge and pressure gauge on the system as seen in the pictures. Currently no heat exchanger, and with the moderate welding I do at the house, I have not had a need for one yet. I may plumb a transmission/oil bar & plate cooler in line in the future if needed.











  22. #72
    Join Date
    Jun 2006
    Location
    Fayetteville, N.C.
    Posts
    227

    Re: Building A Tig Water Cooler For Dummies!!!

    Code4 very nice build.
    I like it...
    TA 181I
    TA 186
    Torchmate 3 5x10
    Victor A120

  23. #73
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    8,443

    Re: Building A Tig Water Cooler For Dummies!!!

    Name:  image.jpg
Views: 2893
Size:  62.2 KBName:  image.jpg
Views: 2913
Size:  64.9 KBfor my precision tig 225, 3 gallon tank made of 1/8 AL. The welder is louder then the cooling system

  24. #74
    Join Date
    Jun 2015
    Location
    Sacramento, CA
    Posts
    645

    Re: Building A Tig Water Cooler For Dummies!!!

    Here is my DIY water cooler:

    I got a carbonator on Craigslist for $100 that had a Procon series 1 pump with a motor and small stainless steel tank. I rewired the motor to bypass the float switch, and plumbed the output of the pump into my WP20 torch, with a bypass valve back to the tank. The pump I got puts out 190psi, so the bypass valve is a necessity or else I will blow the lines off my torch. I usually run the cooler and 55-60psi, and that gives me about 0.5-0.75gpm. I plumbed the return line through a transmission cooler with a big muffin fan, and that keeps the warm water from the torch nice and cool. Most of the plumbing is done with the 3/8" transmission soft line that came with the trans cooler, except for the clear return hose. I used Parker 1/4 npt hydraulic fittings (BHS-60, and BH2-61) to connect to the torch. Using the hydraulic fittings that are double shutoff, the water in the torch lines doesn't drain out when the torch is disconnected from the cooler.

    The first version of the cooler used the stock stainless tank, but now that I have a AC/DC tig welder, I made my own tank from aluminum. It only holds about 0.65-0.7 gallons, but the transmission cooler and high flow fan help keep everything cool. Also my welder only puts out 200A, so I think it is more than enough for my applcation. I also made a steel frame out of 1" .090 wall square tube so everything is protected and somewhat portable. I painted it yellow to match my welder.

    List of parts:
    -Carbonator assembly - Craigslist
    -Brass fittings - Home Depot/Harbor Freight
    -Trans cooler - Oreilly Auto Parts
    -Muffin Fan - Scrap from work
    -4" wide 1/8" aluminum flat bar - metal supply
    -1" .090 wall square tube - metal supply
    -toggle switches - ACE Hardware

    Link to more pics: http://imgur.com/a/qXEDE




    Last edited by njs552; 09-18-2015 at 11:39 PM.
    1988 Big 50 Diesel CC/CV
    1982 Weldanpower 225/210
    1968 SAE 300 motor generator
    Maxstar 200SD
    2015 AHP 200x

    "The trouble with our Liberal friends is not that they're ignorant; it's just that they know so much that isn't so." - Ronald Reagan

  25. #75

    Re: Building A Tig Water Cooler For Dummies!!!

    Have you plumbed a lot of hydraulic lines in your day? Stauff clamps? Very nice job. Thanks for sharing with us.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement