    I have a powermax1250 hooked up to a plasmacam,recently while cutting the machine will move over and pierce hole . However when it starts to move it does not cut through piece.At first it just did it now and then but now it pierces hole but never cuts through.I have taken powerrmax off plasmacam,and used torch manually and it cuts fine.I have also changed my consumables but cannot get it to cut at all when hooked up to plasmacam....any suggestions????

  2. #2
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    9,156

    Re: questions about plasma cam

    LoL!!!!!

    I have that same exact setup, sans DHC.

    So what you are saying is it will not pierce? Because that is what you have to do before cutting starts. Check you amps, pierce time, cut distance, and cut speed and report back.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Th ermalArc400GTSW,LincolnSW2002ea., MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig4ea,MigMax1ea.

  3. #3
    Join Date
    Oct 2007
    Location
    New Hampshire
    Posts
    3,278

    Re: questions about plasma cam

    -Could be a disconnected or poorly connected work cable. Try connecting directly to the material.
    -Torch could be too high off the material.....double check cut charts in operators manual and settings for pierce height and cut height.

    Jim Colt Hypertherm

    Quote Originally Posted by regi245550@gmail.com View Post
    I have a powermax1250 hooked up to a plasmacam,recently while cutting the machine will move over and pierce hole . However when it starts to move it does not cut through piece.At first it just did it now and then but now it pierces hole but never cuts through.I have taken powerrmax off plasmacam,and used torch manually and it cuts fine.I have also changed my consumables but cannot get it to cut at all when hooked up to plasmacam....any suggestions????

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement