Starcut plasma cutter
RSS | Subscribe | Contact Us | Advertise | About Us
Results 1 to 4 of 4
  1. #1
    Join Date
    Sep 2014
    Posts
    119

    Starcut plasma cutter

    Just wondering what comments someone who used one of these might have. They're getting old but my other powcon is such a beast that I keep pondering whether a starcut might be worth picking up. Comments?

    Throwing good money after bad vs digging deeper and getting an equivalent stand-alone hypertherm?

    If you have a line on a decent deal for one, let me know.

    Someone got a screaming deal here http://www.liveauctionworld.com/PowC...rcut_i19619500 105 bucks at auction. I would have been on that all day long, even if it had problems.

  2. #2
    Join Date
    Sep 2008
    Location
    SF bay area, CA
    Posts
    2,845

    Re: Starcut plasma cutter

    they work ok for what they are. But they are definitely not a modern plasma by any standards. I have two of them... they work fine for severing material.
    Vantage 500's LN-25's, VI-400's, cobramatics, Miller migs, synch 350 LX, Powcon inverters, XMT's, 250 Ton Acurrpress 12' brake, 1/4" 10' Atlantic shear,Koikie plasma table W/ esab plasmas. marvel & hyd-mech saws, pirrana & metal muncher punches.

  3. #3
    Join Date
    Mar 2010
    Location
    Ceres, California
    Posts
    3,391

    Re: Starcut plasma cutter

    If you can get consumables. they will ware out twice a fast as a new hypertherm.
    Plus they are picky on what welder you use to power them. 3phase or inverters work best.
    Last edited by ccawgc; 08-09-2015 at 06:38 PM.

  4. #4
    Join Date
    Nov 2015
    Posts
    76

    Re: Starcut plasma cutter

    I just picked one up I think I paid 175. It was a bundle deal. Only tried it once and it seems to cut great. Heres a pic of the one I just got. Name:  image.jpg
Views: 159
Size:  77.5 KB
    Miller Dialarc HF
    Hobart Ironman 230
    Lincoln LN-25
    Powcon Starcut
    Lincoln Weld Pac 100
    Oxy/Acetylene
    '49 SA200 shorthood project

Posting Permissions

  • You may not post new threads