    J-Bevel geometrical configuration

    Hello Dears
    I want to make a wps and design a j-bevel for automatic orbital welding.
    I would appreciate if someone give me a clue how can I do it? is there any Standard that could help me for joint configuration?
    Any answers would be highly appreciated.
    Regard

  2. #2
    Join Date
    Jul 2014
    Location
    MetalTown, USA
    Posts
    1,057

    Re: J-Bevel geometrical configuration

    the code to which your joint has to conform should give you a pretty good start.

    check your code book.
    AWS CWI xxxx2171
    1968 SA200

    Quote Originally Posted by WelderMike
    I hate being bipolar, It's awesome.
    Quote Originally Posted by ZTFab View Post
    Nice work!
    Visit Regulator and Torch Exchange, Inc. for all your cutting and heating needs!

  3. #3
    Join Date
    Sep 2012
    Location
    Wheatland, Wyoming
    Posts
    333

    Re: J-Bevel geometrical configuration

    Look at the AWS standards. They will get you started on what and how you can develop a WPS for your process.
    Chris
    Auction Addict

  4. #4
    Join Date
    Aug 2008
    Posts
    11,095

    Re: J-Bevel geometrical configuration

    "Any day above ground is a good day"

    http://www.farmersamm.com/

  5. #5
    Join Date
    Aug 2008
    Posts
    11,095

    Re: J-Bevel geometrical configuration

    Quote Originally Posted by milomilo View Post
    Look at the AWS standards. They will get you started on what and how you can develop a WPS for your process.
    We discussed the 'J Groove', 'J Bevel' a bit ago. I'm thinking we were discussing a REVERSE J BEVEL Hell, what do I know

    For those not privy to the conversation...…………..

    I was waxing philosophical about welding into a shoulder formed by square tubing, and a flat piece of steel.

    A one shot deal with wire. Single pass fills it up nicely.

    Name:  heat and beat14.jpg
Views: 179
Size:  119.1 KB Some gasless flux core wire. My favorite process Single pass.

    Then you do the real deal, and weld it up with 7018, and now you're looking at 2 passes.

    Name:  heat and beat15.jpg
Views: 180
Size:  117.6 KB Tight root pass to fill the bottom of the void, then a cover pass to fill it on out, both passes using same filler (7018). 7018 is way to "runny" to do it in one pass, and not have a mess...…..too long a dwell time on a 2G weld to fill a deep gap.

    Of interest were the heat signatures. Both came out ok. I was surprised. I don't like wire.

    Name:  heat and beat18.jpg
Views: 178
Size:  132.2 KB 7018

    Name:  heat and beat19.jpg
Views: 181
Size:  112.7 KB Blue Demon equivalent to NR-211

    Looks good on the 11ga material, but I couldn't see inside the square tubing to see just how well the wire did on the thicker material. So, the jury is still out I guess. Which means I can still say bad things about wire
    "Any day above ground is a good day"

    http://www.farmersamm.com/

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement