Anyone familiar with the Boss VXT?
I am replacing my A - Frame, not repairable and $300 and change for a new one is money well spent.
However, the bushing the pin slides through to hold the A-Frame to the center section appears to have a partially cracked weld. I was thinking of grinding out the old weld where its broke and re-welding while the pin is inserted to keep it aligned. Make sense? Or do I repair the weld without the pin in and then ream?