    Re: Rafting Trailer Build

    Quote Originally Posted by WeldedSpoon View Post
    Thanks! I agree, I am happy with it over all, the cross member i mention above and not flat any more when are sprung upward when the trailer is on it's wheels. Maybe i can just call it pre-camber for added load capacity.
    Now you're thinking like a professional welder/ fabricator.

  2. #27
    Join Date
    Apr 2018
    Posts
    17

    Re: Rafting Trailer Build

    So I am getting close to completing this trailer, here are some current pics of progress. Headed out this weekend for it's maiden voyage.
    Name:  20180506_154641.jpg
Views: 130
Size:  101.1 KB
    Name:  20180514_194617.jpg
Views: 130
Size:  74.1 KB
    Name:  20180514_214741.jpg
Views: 130
Size:  56.9 KB
    Name:  20180514_185135.jpg
Views: 130
Size:  52.4 KB
    Name:  20180514_214648.jpg
Views: 130
Size:  59.1 KB

  3. #28
    Join Date
    May 2012
    Location
    north east, PA
    Posts
    398

    Re: Rafting Trailer Build

    Quote Originally Posted by WeldedSpoon View Post
    Attachment 1686058

    Attachment 1686061

    Any help would be appreciated!
    Weld in the top left of the first pic looks questionable, especially for what is doing.

    2nd pic. I personally feel center of a tube for a single gusset like you have is the wrong place for them. The middle of the tube is the weakest spot, if the upright tube does decide to flex and utilize the gusset you put all that stress into that weak spot and the area is prone to cracks. A better place is on the side of the tube for a single gusset, although this looks goofy IMO. I would have most likely cut a piece of tubing on a 45 and welded that in there. Also no need to weld across the tubing, just down the sides. Welding across the tubing ties it into the weak part and gives an area for cracks to form. I am sure some have a different view on this so take it for what it is worth.

  4. #29
    Join Date
    Apr 2018
    Posts
    17

    Re: Rafting Trailer Build

    Quote Originally Posted by Oxford View Post
    Weld in the top left of the first pic looks questionable, especially for what is doing.

    2nd pic. I personally feel center of a tube for a single gusset like you have is the wrong place for them. The middle of the tube is the weakest spot, if the upright tube does decide to flex and utilize the gusset you put all that stress into that weak spot and the area is prone to cracks. A better place is on the side of the tube for a single gusset, although this looks goofy IMO. I would have most likely cut a piece of tubing on a 45 and welded that in there. Also no need to weld across the tubing, just down the sides. Welding across the tubing ties it into the weak part and gives an area for cracks to form. I am sure some have a different view on this so take it for what it is worth.
    Thanks for the input.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement