    Only been tig welding a couple of years. Have gotten fairly good most of the time. Recently the welds have gotten pretty weird. Would go along ok one day and go south the next. Attached is a picture of what the weld looks like. Everthing looks ok when welding but looks like this when done. Machine or Me?Name:  IMG_1158.jpg
Views: 169
Size:  67.1 KB

  2. #2
    Join Date
    Oct 2014
    Posts
    222

    Re: Diversion 180 problem

    It might just be junk pulling into the weld from the I.D. or O.D. of the tubing slipped together. Exhaust tubing I guess. ?? was either previously a used piece ?
    Try a flat weld on two clean pieces of other steel and see if it will weld clean and you will know if it something else.

  3. #3
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    8,603

    Re: Diversion 180 problem

    Looks like a gas issue.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Th ermalArc400GTSW,LincolnSW2002ea., MillerMatic350P,MillerMatic200withspoolgun,MKCobra Mig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig3ea.

  4. #4
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    6,330

    Re: Diversion 180 problem

    Welcome to the forum

  5. #5
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    4,887

    Re: Diversion 180 problem

    Weld a bead lengthwise down a piece of that pipe. If that is clean, try a butt weld. I'd guess gas coverage issue. You have some unpredictable air current coming in from the gap in the joint, or it's dirty inside the joint. Diversion 180 should weld steel just fine. DCEN, Pure argon, tank not near empty, torch close, held at a steep angle. You might try a gas lens. It diffuses gas as a kitchen sink aerator does, I almost always use one. 15-20 CFH.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  6. #6
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    6,330

    Re: Diversion 180 problem

    Don't see how it could be incoming air from the pipe unless he's got a blow gun in the tube.guys make open root pipe welds all day

  7. #7
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    8,603

    Re: Diversion 180 problem

    Aircooled torch combined with cheap chinese collets creates crushed collets and gas blockage. First thing I do every morning is confirm gas flow with my portable gas flowchecker.
    Name:  Torch_with_PFM.jpg
Views: 80
Size:  3.8 KB

    After confirming proper gas flow I pull out my trusted ER312 for difficult welds or dissimilar metals.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Th ermalArc400GTSW,LincolnSW2002ea., MillerMatic350P,MillerMatic200withspoolgun,MKCobra Mig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig3ea.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement