    Re: Bobcat 225g Idle Solenoid

    Duane you are a genius! Ran a switched 12v wire to H terminal and it works perfect. Excites to high idle like it should and everything. Once again thanks for all your help

  2. #27
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    16,642

    Re: Bobcat 225g Idle Solenoid

    I should have clarified but I believe you can just jumper from terminal B to terminal H and not include an additional switch in the picture.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  3. #28
    Join Date
    Mar 2018
    Posts
    23

    Re: Bobcat 225g Idle Solenoid

    I actually didn't run an extra switch, just jumped off of a open spade terminal on S-2. Good for anyone else to know that you can make the cheaper module work, saves a few hundred $

  4. #29
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    16,642

    Re: Bobcat 225g Idle Solenoid

    IIRC, I've seen photos of that module with a tandem QD spade terminal jumper included to go between B & H.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement