    XR-30 Feeder Compatibility

    Got a chance to pick up a XR-30 Wire feeder and gun at a good price. Just need to know if I can use it with my Shopmaster 300.

    Thanks

  2. #2
    Join Date
    Nov 2014
    Posts
    281

    Re: XR-30 Feeder Compatibility

    Just an FYI follow-up on this post. The XR-30 and XR wire feeder work with the Shopmaster 300.