    I’m going to look at buying a used 12vs extreme rigged up currently for .052 flux core wire. I’m going to try it off my 305g. What settings should I try? Also, I’ll be testing it in a scrap piece of 4” channel. How many amps should I try it at? I’ve ran several pounds of wire before. Mostly .30, .35, and .45. Never ran .052, so I was looking for a starting point. Thanks.

  2. #2
    Join Date
    Oct 2015
    Posts
    1,729

    Re: Miller 12vs .052 flux wire

    Who ever makes your .052 wire should have setup specs on their web site. I run .045 flux core in my 12vs. I run Hobart 21B most of the time. I run around 18-19V and about 160 ipm with it unless I am on real thin material then I go to 17V and around 120IPM. I would guess you are going to be in the 18-21V range and 100 to 150 IPM but that is only a guess. Make sure to switch polarity to run the flux core.

    FYI ; Some flux core wire is moisture sensative and if it is old wire it might not run well no matter what. That is one reason I run the H21B it does not seem to be effected by moisture very much. I am running a 30 lb roll in it now that is about a year old and runs fine.
    Last edited by thegary; 05-13-2018 at 07:44 PM.

  3. #3
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    1,691

    Re: Miller 12vs .052 flux wire

    When in doubt with fluxcore... start with the wire speed high and turn it down to get a smooth arc. It will save a ton of tips ruined from burn back.
    I haven't used my 12VS for a few months, but it seems to me that on CV the wire speed control is kind of backwards, meaning more wire for a lower voltage setting. And the manual was absolutely zero help, 33 pages of safety warnings but it really never tells you how to use it.

  4. #4
    Join Date
    Feb 2011
    Posts
    133

    Re: Miller 12vs .052 flux wire

    Bought it for $525. The 12vs has a 400 amp Profax Mig gun, running ESAB dual shield 2 70t-12h4. Has .045 rollers too. Ran it for a few minutes without gas just to see if it was welding. Ran pretty good, except for the porosity on starts and stops. But I’m sure that’s because the lack of shielding gas. Going to try running a 75/25 mix tomorrow. What would be a good flux gun to buy? I’m thinking about getting a 300amp since neither of my 3 machines will put out more than around 300 amps. I will be running a 305g, miller big 20, or a Bobcat 225. I mainly run weld on 3/8-3/4 steel. Any suggestions? What’s a good wire to run? I use Hobart .035 Mig wire on the 110 machine with good luck.

  5. #5
    Join Date
    May 2018
    Location
    Iowa,Des Moines
    Posts
    4

    Re: Miller 12vs .052 flux wire

    When I bought the Trailblazer 302, I asked everyone about a Suitcase -- VS or RC. Although the VS will work on the 302, every opinion I got was to buy the RC.

    Disadvantage - it uses a Remote Control cable.

    Advantage - Wire feeding is more consistent, even at low voltages

    The 12RC combined with the 302 will amaze you with its smoothness. You may want to try one before you buy the VS.

  6. #6
    Join Date
    Oct 2015
    Posts
    1,729

    Re: Miller 12vs .052 flux wire

    nothing wrong with a 12vs at all. I run mine on a TB302 and have never had a problem.

  7. #7

    Re: Miller 12vs .052 flux wire

    Quote Originally Posted by thegary View Post
    nothing wrong with a 12vs at all. I run mine on a TB302 and have never had a problem.
    I have used 1,000'S pound o52 wire
    I side for work I was doing

    Dave

    Sent from my SAMSUNG-SM-J320A using Tapatalk
    HF 170 welder
    HF 4x6 band saw
    South Bend 9N
    Mill
    B&D mag drill
    Victor torch

  8. #8
    Join Date
    Jun 2015
    Location
    Sacramento, CA
    Posts
    644

    Re: Miller 12vs .052 flux wire

    12vs will work fine for you. I use an LN-25, but that's only because I happened across it for a good price.

    As for self-shielded wire, I use Lincoln NR-232 or Esab Coreshield 8/Lincoln Nr-233. 062-078(5/64) diameter wires. Runs somewhere north of 200 amperage wise @ ~20v and ~120 ipm.

    Be advised there is a bit of a learning curve with those T-8 wires I mentioned. Once you've got it figured out it's one of the fastest ways to weld 3/8"+ metal out in the field.

    Sent from my SM-G960U using Tapatalk
    Last edited by njs552; 05-14-2018 at 02:39 PM.
    1988 Big 50 Diesel CC/CV
    1982 Weldanpower 225/210
    1968 SAE 300 motor generator
    Maxstar 200SD
    2015 AHP 200x

    "The trouble with our Liberal friends is not that they're ignorant; it's just that they know so much that isn't so." - Ronald Reagan

  9. #9
    Join Date
    Feb 2011
    Posts
    133

    Re: Miller 12vs .052 flux wire

    Actually had some time to fool with it. Got the .052 Esab dualshield to run great. But only in a flat position. I didn’t have the hardware to run .030 solid wire, but I have it a try anyway. It actually fed really well and ran like a champ. I’m ordering the right consumables and .045 solid Mig wire so I can get more time on it. I’m really impressed with the 305g’s mg capabilities.

  10. #10
    Join Date
    Apr 2010
    Location
    The Peoples Republic of Kalifornia
    Posts
    3,261

    Re: Miller 12vs .052 flux wire

    I have both the 12 RC which i bought first and yes it is better at somethings like what i used it for at the time which was body work and other mig type work
    running the .030 and .035 wire and into .045 stuff using it for spray it does a great job

    But eventually i had to cut the cord which was never long enough to do somethings
    Bought the 12 VS so i could do the other things i needed to do on heavy equipment and other install type work that took me to over 75 ft length of the RC control cable

    On equipment repair work i run a lot of Lincoln outershield 71-m and elite in .045 and .062 and for the real big stuff i run the esab core shield 8 in 0.72 self shield wire
    The 12 VS works just fine for all i do now the 12 RC is just a dust collector now ..Because seriously dragging all that cable around is a drag and i don't do body work anymore
    Backed my CATMA over your CARMA oops clusmy me

    What would SATAN do ??


    Miller Trailblazer 302 AirPak
    Miller Digital Elite
    Optrel Welding Hat
    Arcair K4000
    Suitcase 12RC / 12 VS
    Hypertherm PM-45
    Rage 3 saw
    Rusty old Truck

  11. #11
    Join Date
    Feb 2011
    Posts
    133

    Re: Miller 12vs .052 flux wire

    It ran well on the 305g in cv mode, but it ran exceptionally well on my big 20 in cc mode. Bought the right tips today, ordered .045 er70s-6, .045 tweeco tips, and the right rollers. I’ll be set soon. Thanks for the help.

  12. #12
    Join Date
    Feb 2011
    Posts
    133

    Re: Miller 12vs .052 flux wire

    What’s a good alternative to the Bernard duraflux gun the 12vs is sold with?

  13. #13
    Join Date
    Feb 2011
    Posts
    133

    Re: Miller 12vs .052 flux wire

    I just bought a Bernard duraflux gun for the 12vs. It runs 1/16th-5-64th wire. I weld a lot of 3/8-1/2”. What would be a good 1/16th wire for welding structural? Mainly I beams and plate. Some pipe as well. I was thinking of Esab Coreshield, or Hobart 21b.

  14. #14
    Join Date
    Oct 2007
    Location
    Vandalia, Ohio near Dayton
    Posts
    2,473

    Re: Miller 12vs .052 flux wire

    Quote Originally Posted by diesel625 View Post
    I just bought a Bernard duraflux gun for the 12vs. It runs 1/16th-5-64th wire. I weld a lot of 3/8-1/2”. What would be a good 1/16th wire for welding structural? Mainly I beams and plate. Some pipe as well. I was thinking of Esab Coreshield, or Hobart 21b.
    Hobart XLR-8 is a solid product for structural work. Like ESAB Coreshield 8 and the equivalent Lincoln NR233. All 3 meet D1.8 for structural work with seismic requirements. All 3 weld just a bit differently than a lot of guys are accustomed to. If you pick the HObart wire I recall there's a demo video on their website that shows proper technicque for XLR-8.

    Hobart 21B is excellent for general purpose work and non-critical structural work. But wouldn't be my choice for weldments requiring high toughness at low temps.
    Benson's Mobile Welding at your worksite or place of business. Serving Dayton, Ohio and the surrounding metro areas.
    AWS Certified Welding Inspector (#XXX10731) and Certified Welding Educator (#XXX1008E)

  15. #15
    Join Date
    Feb 2011
    Posts
    133

    Re: Miller 12vs .052 flux wire

    Ok. What about Coreshield 11? I read it’s not for jobs with seismic requirements, which would be fine for what I’m going to use it for. How does it run compared to coreshield 8?

  16. #16
    Join Date
    Jun 2015
    Location
    Sacramento, CA
    Posts
    644

    Re: Miller 12vs .052 flux wire

    Esab Coreshield 11, Lincoln NR211 and Hobart 21b all fall under the t-11 classification. They run really smooth, but if your welding to code they have seismic and thickness limitations.

    Esab Coreshield 8 / Lincoln NR-233 and Nr-232 all fall under the t-8 classification. They meet all seismic requirements and do not have thickness limitations.

    The t-8 wires will also deposit about 50% more weld per hour. 2-8lb/hr for .068 NR-211 vs 4-12lb/hr on the .068 NR232. Depends on settings of course.

    Sent from my SM-G960U using Tapatalk
    1988 Big 50 Diesel CC/CV
    1982 Weldanpower 225/210
    1968 SAE 300 motor generator
    Maxstar 200SD
    2015 AHP 200x

    "The trouble with our Liberal friends is not that they're ignorant; it's just that they know so much that isn't so." - Ronald Reagan

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement