    How to mix helium and argon

    I'm getting into 1/4" to 3/4" aluminum and need to mix some helium with the argon. What do I need as far as gauges and flow meters? How do you combine the two gases to one welder?

  2. #2
    Join Date
    Mar 2017
    Location
    bar stool
    Posts
    660

    Re: How to mix helium and argon

    You buy an older Smith (Pre ITW) gas mixer for Argon Helium and hook it up.

    There are minimally 7,953 other ideas how to do it on the inTurdnet. NONE work like a gas mixer does.

  3. #3
    Join Date
    Feb 2012
    Location
    Hell I see Sparks
    Posts
    3,634

    Re: How to mix helium and argon

    Quote Originally Posted by PorkBarrel View Post
    I'm getting into 1/4" to 3/4" aluminum and need to mix some helium....

    How do you combine the two gases to one welder?

    Victor style WYE

  4. #4
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    2,630

    Re: How to mix helium and argon

    The Smith gas mixer is the only way to do it with any sort of accuracy. The wye method is just a guessing game, repeatability and accuracy are questionable at best. Otherwise, just buy the gas mix you need.

  5. #5
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    8,603

    Re: How to mix helium and argon

    Quote Originally Posted by walker View Post
    The Smith gas mixer is the only way to do it with any sort of accuracy. The wye method is just a guessing game, repeatability and accuracy are questionable at best. Otherwise, just buy the gas mix you need.
    "Y" method is called blending.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Th ermalArc400GTSW,LincolnSW2002ea., MillerMatic350P,MillerMatic200withspoolgun,MKCobra Mig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig3ea.

  6. #6
    Join Date
    Mar 2014
    Posts
    4,440

    Re: How to mix helium and argon

    Porky,

    Here's how I'm set up to get some Helium blended into my Argon to help out welding heavier aluminum. All it takes is a little bit of playing around and you'll find where you want your flow meters set. Since Helium is so expensive you want to try and use as little of it as necessary.

    Also, you don't need a wye connector with valves on it like you see in the picture. That's just what I already had on hand.

    Name:  10 16 11 004.jpg
Views: 229
Size:  91.5 KB

  7. #7
    Join Date
    May 2010
    Location
    Sparks, NV
    Posts
    9,363

    Re: How to mix helium and argon

    If you find an argon CO2 Smith mixer, her is the conversion chart for argon helium
    Tiger Sales: AHP Distributor www.tigersalesco.com
    AHP200x; AHP 160ST; MM350P, Spoolmatic 30A; Everlast PowerTig 185; ESAB 875 plasma;Evo 355. OA

  8. #8
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    3,807

    Re: How to mix helium and argon

    Rent a cylinder that already mixed.

  9. #9
    Join Date
    Mar 2017
    Location
    Sierra Mountains
    Posts
    17

    Re: How to mix helium and argon

    Quote Originally Posted by walker View Post
    The Smith gas mixer is the only way to do it with any sort of accuracy. The wye method is just a guessing game, repeatability and accuracy are questionable at best. Otherwise, just buy the gas mix you need.
    Jody suggested getting the gas mix 50/50 that way I can utilize flow meter for both. Another one also mentioned. Thanks for all the great ideas!

  10. #10
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    8,603

    Re: How to mix helium and argon

    Quote Originally Posted by PorkBarrel View Post
    Jody suggested getting the gas mix 50/50 that way I can utilize flow meter for both. Another one also mentioned. Thanks for all the great ideas!
    Yes. set your argon flow at your desired half, then add enough helium to flow the other half. As long as you confirm the total you should be good. Actually I go 50/50 at the flowmeters, then confirm total at the torch.

    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Th ermalArc400GTSW,LincolnSW2002ea., MillerMatic350P,MillerMatic200withspoolgun,MKCobra Mig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig3ea.

  11. #11
    Join Date
    Mar 2017
    Location
    Sierra Mountains
    Posts
    17

    Re: How to mix helium and argon

    Thanks. I printed and will use as reference.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement