    Process for padding beads?

    How many beads do you run before you cool the pad off and clean off the slag? The idea of running one 4 - 6" bead, cooling it off, wire brushing the slag, then starting the next bead is rather daunting. It would take forever to fill a 6 x 6 pad.

    The whole point as I see it is to build control and muscle memory but if you have a prolonged stop after every bead is that accomplishing what you're after? I've been running bead after bead until they start running funny when the pad gets too hot before I cool it off and wire brush the slag but am wondering if that's a bad method?

  2. #2
    Join Date
    Jul 2011
    Location
    Bossier Parish La.
    Posts
    5,187

    Re: Process for padding beads?

    One thing you can do is use 4 or more of the 6x6 pads clamped to a longer piece of steel and run one bead on each one. Then go back and chip/brush off the slag and run another bead on each. This gives each pad a chance to cool off on it's own some between beads. When they all seem to be too hot, hose them all off to cool and start over. Using just the one pad concentrates all the heat into just that one with no time in between for any cooling to take place. If they are all clamped to a thick piece of steel, that can help act as a heat sink too, to draw out heat faster between beads.

  3. #3
    Join Date
    Jun 2012
    Location
    Bemidji MN
    Posts
    13,399

    Re: Process for padding beads?

    Use longer plates - 12" to 24" long.

    Way more time welding that way in my opinion.

    Little plates just heat up too fast.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  4. #4
    Join Date
    Nov 2012
    Location
    South Texas
    Posts
    2,248

    Re: Process for padding beads?

    Buy more plates. :idea:

  5. #5
    Join Date
    Oct 2011
    Location
    Jacksonville Florida
    Posts
    2,339

    Re: Process for padding beads?

    Larger plate like Dave said... part of the reason to do this exercise is to learn to weld. If you don't stop to clean and inspect each weld to see if you're doing things right then you can't improve.
    Airco Ac/Dc 300 Heliwelder
    MillerMatic 200
    Miller Maxstar 150STL

  6. #6
    Join Date
    Mar 2014
    Posts
    4,440

    Re: Process for padding beads?

    I also think having multiple plates is a good idea. Possibly a little thicker also (say 3/8 vs. 1/4).

    When it comes to quenching your plate off....give it repeated quick dips and try and leave enough heat in it that it'll steam itself off dry in 30 seconds or less after the last dip. Then just give it a quick rake with your de-slagging tool of choice, and a token wire brushing and put another bead (or three) on it. It's padding practice not a code groove weld that's going to get x-rayed.

  7. #7
    Join Date
    Jan 2015
    Location
    Ohio
    Posts
    365

    Re: Process for padding beads?

    I started wondering about the process when I saw padding practice on youtube (Jody and others) and good padding samples on here. All were on relatively small plates, maybe the 6" size I mentioned. And all the ones I remember looked really good, like someone ran one bead, cooled it off, brushed the slag then carefully laid another one halfway on the first. So I thought "wow, if that's how it's supposed to be done I must be doing it wrong." and thought I'd ask.

  8. #8
    Join Date
    Mar 2018
    Location
    Tampa, Florida
    Posts
    442

    Re: Process for padding beads?

    As a new guy that’s been doing a bunch of pads. I’ve been running 1/8” rod on 3/8” A36 plates. Usually 6x6 or 10x10”. Idea overlap is 1/3rd bead width I’ve been told, it is a good idea to cool off every few. I did some non cooled pads, and as rigid as a piece of 6x6” 3/8” steel plate is, heat will curl it like a potato chip. Also excessively hot metal holds on to slag more aggressively, which means more time chipping and brushing those last few pieces.
    -Mark Smith

    Vulcan ProTig200
    Vulcan MigMax 215

  9. #9
    Join Date
    Mar 2014
    Posts
    4,440

    Re: Process for padding beads?

    Quote Originally Posted by JD1 View Post
    I started wondering about the process when I saw padding practice on youtube (Jody and others) and good padding samples on here. All were on relatively small plates, maybe the 6" size I mentioned. And all the ones I remember looked really good, like someone ran one bead, cooled it off, brushed the slag then carefully laid another one halfway on the first. So I thought "wow, if that's how it's supposed to be done I must be doing it wrong." and thought I'd ask.
    JD1,

    It certainly wouldn't hurt to have something bigger than 6" to practice on. In fact if you had something big enough that you couldn't get all the way across it with one rod you get more practice at restarting welds and getting a smooth transition from one bead to the next.

    What size and shape material you're running beads on is not as important as to just keep running beads on something.

    If you can find a piece of heavy angle iron you can start practicing laying up multi pass fillet welds. If you fill something like this even half way you get a lot a practice.

    Name:  7018 028.jpg
Views: 194
Size:  110.3 KB

  10. #10
    Join Date
    Mar 2014
    Posts
    4,440

    Re: Process for padding beads?

    How's this for some serious horizontal padding practice?

    Name:  P03-04-09_14.29[01].jpg
Views: 182
Size:  136.3 KB

    Name:  P03-04-09_16.57.jpg
Views: 183
Size:  82.8 KB

  11. #11
    Join Date
    Jun 2012
    Location
    Bemidji MN
    Posts
    13,399

    Re: Process for padding beads?

    Quote Originally Posted by HT2-4956 View Post
    How's this for some serious horizontal padding practice?

    Name:  P03-04-09_14.29[01].jpg
Views: 182
Size:  136.3 KB
    Appears to meet minimum acceptable guidelines to pass visual
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  12. #12
    Join Date
    Jan 2015
    Location
    Ohio
    Posts
    365

    Re: Process for padding beads?

    Quote Originally Posted by HT2-4956 View Post
    JD1,
    In fact if you had something big enough that you couldn't get all the way across it with one rod you get more practice at restarting welds and getting a smooth transition from one bead to the next.
    Good idea. Turns it into more than just running rows of beads. I'll do that.

  13. #13
    Join Date
    Mar 2018
    Posts
    27

    Re: Process for padding beads?

    In my class they have us run a bead, stop clean inspect reason what your doing wrong and then run the next with overlap. This gives a little time for cooking, we quench about every 3 beads with the size we use. Take it for what's it worth, I cant if it's right or wrong but that's what my instructor has us do.

    Sent from my SM-N950U using Tapatalk

  14. #14
    Join Date
    Apr 2008
    Location
    NW ON Canada
    Posts
    2,960

    Re: Process for padding beads?

    [/QUOTE]The whole point as I see it is to build control and muscle memory but if you have a prolonged stop after every bead is that accomplishing what you're after? I've been running bead after bead until they start running funny when the pad gets too hot before I cool it off and wire brush the slag but am wondering if that's a bad method?[/QUOTE]

    The hole point of padding beads is to learn/practice what drag angle, work angle, arc length, travel speed, electrode manipulation and selected welding amperage does to your bead.



    Sent from my iPhone using Tapatalk
    Jason
    Lincoln Idealarc 250 stick/tig
    Thermal Dynamics Cutmaster 52
    Miller Bobcat 250
    Torchmate CNC table
    Thermal Arc Hefty 2
    Ironworkers Local 720

  15. #15
    Join Date
    Jun 2012
    Location
    CT
    Posts
    3,038

    Re: Process for padding beads?

    The whole point as I see it is to build control and muscle memory but if you have a prolonged stop after every bead is that accomplishing what you're after?
    That's probably not the point. The point (IMO) is to practice, with extreme intention on every bead, so that you learn. if you are making mistakes while you build muscle memory you aren't doing yourself any good.You can't practice with intention if you are not removing slag and inspecting the bead each time. Again, IMO.
    Millermatic 252
    Syncrowave 250
    Purox Metalmaster

  16. #16
    Join Date
    Jan 2015
    Location
    Ohio
    Posts
    365

    Re: Process for padding beads?

    Quote Originally Posted by HT2-4956 View Post
    How's this for some serious horizontal padding practice?

    Name:  P03-04-09_14.29[01].jpg
Views: 182
Size:  136.3 KB

    Name:  P03-04-09_16.57.jpg
Views: 183
Size:  82.8 KB
    That looks like roughly a 6" pad. What was your process? Run one bead, de-slag, repeat 2 or 3 times, quench, then do more?
    Last edited by JD1; 05-20-2018 at 07:39 AM.

  17. #17
    Join Date
    Mar 2014
    Posts
    4,440

    Re: Process for padding beads?

    Quote Originally Posted by JD1 View Post
    That looks like roughly a 6" pad. What was your process? Run one bead, de-slag, repeat 2 or 3 times, quench, then do more?
    One of the tricks to getting a nice horizontal pad built up quickly is to not chip your slag after each rod. The slag on the previous (lower) bead gives you more of a shelf to set the next bead on. You can run a heavier bead that way with out it sagging. You start at the bottom and work up until you have a layer on and then you chip and wire brush that whole layer before starting the next layer.

    There was no "quenching" involved. In fact there was a 400 F. preheat maintained on that while welding. There's enough mass there that the part getting over heated wasn't a problem.

  18. #18
    Join Date
    Mar 2014
    Posts
    4,440

    Re: Process for padding beads?

    Quote Originally Posted by Mmock4 View Post
    As a new guy that’s been doing a bunch of pads. I’ve been running 1/8” rod on 3/8” A36 plates. Usually 6x6 or 10x10”. Idea overlap is 1/3rd bead width I’ve been told, it is a good idea to cool off every few. I did some non cooled pads, and as rigid as a piece of 6x6” 3/8” steel plate is, heat will curl it like a potato chip. Also excessively hot metal holds on to slag more aggressively, which means more time chipping and brushing those last few pieces.
    The solution to that is to alternate sides. After you get one layer on the first side put the next 2 layers on the other side and then alternate back and forth one layer at a time. For that matter you don't even need to put full layers on before switching sides. Weld a few beads on one side to where it gets to hot and needs to be quenched and then after cooling it off flip it over and put the same number of beads just opposite those on the other side. And then just keep flip flopping back and forth like that.

  19. #19
    Join Date
    Mar 2014
    Posts
    4,440

    Re: Process for padding beads?

    With those temporary run out tabs on it and the flame resistant material hung there as screening that first picture is kind of misleading as to the actually mass of the part that's getting welded on. When you have this much mass behind you to suck up the heat from welding getting your part over heated isn't usually a problem. You can usually burn one rod right after the other for hours on end. And when you get to where you're needing a break there's another welder standing by to tag in and keep going at it.

    Name:  P03-04-09_16.53[01].jpg
Views: 94
Size:  105.0 KB

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement