MECO Type O multi seat regulators
RSS | Subscribe | Contact Us | Advertise | About Us
Results 1 to 7 of 7
  1. #1
    Join Date
    Jun 2014
    Location
    Southern Illinois
    Posts
    513

    MECO Type O multi seat regulators

    I've had a set of type O MECO oxy/acetylene regulators for years and they were old when I got them. The other day I noticed the line gauge on the acetylene regulator was creeping up and up with torch valves off. I started exploring repair options, I really didn't want to junk them. I asked around and found a local shop that would look at it. I took it in, he looked it over, went to a vice and removed the cap from the rear of the regulator. He took a screwdriver and removed the seat block that has 4 seats on it. He rotated to a good unused seat and put it all back together. He said I had one more left and then I would need a new seat block. Took about 15 minutes and $10 and I was fixed. I was happy it was simple, did a google search and found advertising from MECO in 1922 touting their multi seat regulators. Are their any others like this? Victor bought MECO in 1999 I guess and phased their products out. Anybody else have any of these?


    Sent from my iPad using Tapatalk
    Steve

    Miller Dialarc 250 (1990)
    Miller Maxstar 140 STR (2003)
    Lincoln SA200 Redface Pipeliner (1966)
    Lincoln MP210 (2015)
    Victor and MECO torches

  2. #2
    Join Date
    Jun 2012
    Location
    Bemidji MN
    Posts
    13,374

    Re: MECO Type O multi seat regulators

    That's really interesting. I didn't know some regulators were made that way.

    Only 8am and I've already learned my "something new" quota for the day
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  3. #3
    Join Date
    Jun 2014
    Location
    Southern Illinois
    Posts
    513

    Re: MECO Type O multi seat regulators

    Glad to help. It was news to me as well. Just in case somebody has the same problem you can fix it yourself. It's not rocket science.


    Sent from my iPad using Tapatalk
    Steve

    Miller Dialarc 250 (1990)
    Miller Maxstar 140 STR (2003)
    Lincoln SA200 Redface Pipeliner (1966)
    Lincoln MP210 (2015)
    Victor and MECO torches

  4. #4
    Join Date
    Jun 2012
    Location
    Bemidji MN
    Posts
    13,374

    Re: MECO Type O multi seat regulators

    I wonder if my old oxygen regulator had something similar. I replaced it when it started to creep.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  5. #5
    Join Date
    Jun 2014
    Location
    Southern Illinois
    Posts
    513

    Re: MECO Type O multi seat regulators

    On the back of both type O regulators it states "multi seat" so the oxygen regulator is the same. Still have it? Tare it down and look


    Sent from my iPad using Tapatalk
    Steve

    Miller Dialarc 250 (1990)
    Miller Maxstar 140 STR (2003)
    Lincoln SA200 Redface Pipeliner (1966)
    Lincoln MP210 (2015)
    Victor and MECO torches

  6. #6
    Join Date
    Jun 2012
    Location
    Bemidji MN
    Posts
    13,374

    Re: MECO Type O multi seat regulators

    I will do that
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  7. #7
    Join Date
    Jun 2014
    Location
    Southern Illinois
    Posts
    513

    Re: MECO Type O multi seat regulators

    Post a picture if you can.


    Sent from my iPhone using Tapatalk
    Steve

    Miller Dialarc 250 (1990)
    Miller Maxstar 140 STR (2003)
    Lincoln SA200 Redface Pipeliner (1966)
    Lincoln MP210 (2015)
    Victor and MECO torches

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement