    Picked up a new welder & also results on a nugget for another machine

    Picked up a Lincoln SP100 for $100 today and couldn't pass it up. Love infinite controls on machines. My Miller 130xp is a tap machine and i needed the SP for light stuff so it worked out great. VERY impressed with how hot it burns for a 100. I never expected it to do as well as it does. Not really useful since it'll be on the cold side when I use it, but dang it gets it when you crank it.

    So anyway while I'm talking mig, i did a nugget test today out of curiosity to see what the XP would do against a 1/4" angle iron. Not too shabby at all stacking a 110v machine against 1/4 angle.







    Last edited by One1; 06-12-2018 at 11:41 PM.
    1957 Lincoln Idealarc 300 AC/DC
    1971 Miller Thunderbolt 225
    2018 Lincoln 180
    2018 Lincoln 3350 papr

  2. #2
    Join Date
    Apr 2018
    Location
    TN
    Posts
    170

    Re: Picked up a new welder & also results on a nugget for another machine

    Tig @150 amps 100% argon. Very disappointing.

    1957 Lincoln Idealarc 300 AC/DC
    1971 Miller Thunderbolt 225
    2018 Lincoln 180
    2018 Lincoln 3350 papr

  3. #3
    Join Date
    Apr 2018
    Location
    TN
    Posts
    170

    Re: Picked up a new welder & also results on a nugget for another machine

    Lincoln SP100. smoking hot on the surface, does a great job on thin material, no match against the 1/4". Conclusively the Miller 130xp is exceptional for a 110v

    1957 Lincoln Idealarc 300 AC/DC
    1971 Miller Thunderbolt 225
    2018 Lincoln 180
    2018 Lincoln 3350 papr

  4. #4
    Join Date
    Apr 2018
    Location
    TN
    Posts
    170

    Re: Picked up a new welder & also results on a nugget for another machine

    After re-etching them I've decided the tig did good

    1957 Lincoln Idealarc 300 AC/DC
    1971 Miller Thunderbolt 225
    2018 Lincoln 180
    2018 Lincoln 3350 papr

  5. #5
    Join Date
    Apr 2018
    Location
    TN
    Posts
    170

    Re: Picked up a new welder & also results on a nugget for another machine

    Hobart 1/8 6011 @130a very pleased. Good rod.

    1957 Lincoln Idealarc 300 AC/DC
    1971 Miller Thunderbolt 225
    2018 Lincoln 180
    2018 Lincoln 3350 papr

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement