Soft copper tube for butt splice
RSS | Subscribe | Contact Us | Advertise | About Us
Results 1 to 13 of 13
  1. #1
    Join Date
    May 2010
    Location
    ct.
    Posts
    973

    Soft copper tube for butt splice

    Anyone ever used soft copper tube for butt splicing
    welding cables?
    One of my cables has a big tape covered knob where
    I spliced it with a split bolt.
    Looking for something smaller than a set screw type
    connector.
    Soft copper tubing,crimped with a hammer type
    swage tool, and covered with heat shrink?
    Miller a/c-d/c Thunderbolt XL
    Millermatic 180
    Purox O/A
    Smith Littletorch O/A
    Hobart Champion Elite

  2. #2
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    1,767

    Re: Soft copper tube for butt splice

    Quote Originally Posted by jpump5 View Post
    Anyone ever used soft copper tube for butt splicing
    welding cables?
    One of my cables has a big tape covered knob where
    I spliced it with a split bolt.
    Looking for something smaller than a set screw type
    connector.
    Soft copper tubing,crimped with a hammer type
    swage tool, and covered with heat shrink?
    I've done it once or twice, even on heavy equipment battery cables as a "get it going" fix. You want a good tight crimp, push the cable together as tightly as possible before the second crimp.

  3. #3
    Join Date
    Jun 2016
    Location
    by a resevior in north central ar.
    Posts
    160

    Re: Soft copper tube for butt splice

    I have and then drilled a 2 small hole in the copper at the crimp and then soldered it. shrink wrap, tape and then covered with wire harness loom cover and taped again

  4. #4
    Join Date
    Apr 2006
    Location
    Soda springs,Id
    Posts
    4,315

    Re: Soft copper tube for butt splice

    Why not just spend the extra $$ and buy a pair of twistlok welding cable connectors??
    Mike
    Ol' Stonebreaker
    "Experience is the name everyone gives to their mistakes"

    Miller 175 mig
    Miller thunderbolt ac/dc stick
    Victor O/A setup
    Makita chop saw

  5. #5
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    916

    Re: Soft copper tube for butt splice

    As long as you don't have to deal with osha it will be fine, those osha people seem to dislike electrical tape on welding leads, extension cords etc.
    NRA LIFE MEMBER
    UNITWELD 175 AMP 3 IN1 DC MIG/STICK/TIG
    MIDSTATES 300 AMP AC MACHINE
    GOD BLESS AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  6. #6
    Join Date
    May 2010
    Location
    ct.
    Posts
    973

    Re: Soft copper tube for butt splice

    Quote Originally Posted by mla2ofus View Post
    Why not just spend the extra $$ and buy a pair of twistlok welding cable connectors??
    Mike
    I thought about that. I’d rather have a permanent connection that’s smaller and cheaper.

    Caveman, if OSHA were ever to inspect my home shop, spliced welding cables would probably be
    one of they’re lesser concerns.
    Miller a/c-d/c Thunderbolt XL
    Millermatic 180
    Purox O/A
    Smith Littletorch O/A
    Hobart Champion Elite

  7. #7
    Join Date
    Apr 2006
    Location
    Soda springs,Id
    Posts
    4,315

    Re: Soft copper tube for butt splice

    You can buy shrinktube that's about as thick as lead insulation.
    Mike
    Ol' Stonebreaker
    "Experience is the name everyone gives to their mistakes"

    Miller 175 mig
    Miller thunderbolt ac/dc stick
    Victor O/A setup
    Makita chop saw

  8. #8
    Join Date
    Mar 2017
    Location
    Forest Grove OR
    Posts
    228

    Re: Soft copper tube for butt splice

    Yes it will work, but cross sectional copper content in the splice will be far less than the 2 conductors being joined, and 100% of the current has to pass through the splice to get from one conductor to the other. Like using a small diameter chain link in-line to join two big chains together. It will work, but you restrict current capacity. In actual use, it acts like an inline resistor, and will likely get warm/hot. Split bolts are ugly, but they bond both conductors directly together and little current goes through the bolt, there is no current capacity loss if the splice is tight.

    This is one of the "correct" in-line ways to do it :

    https://www.amazon.com/Easy-Splice-L.../dp/B008KMKESI

    No cross-sectional loss with a splice like this. You can then heat shrink it.
    Everlast 350 EXT - Thermal Dynamics Cutmaster 52 - Rogue Fabrication M600 xHD tube bender
    Milwaukee 4208 Mag Drill - Shopmaster Eldorado Combo mill/lathe machine with DRO.

  9. #9
    Join Date
    May 2010
    Location
    ct.
    Posts
    973

    Re: Soft copper tube for butt splice

    Quote Originally Posted by Chad86tsi View Post
    Yes it will work, but cross sectional copper content in the splice will be far less than the 2 conductors being joined, and 100% of the current has to pass through the splice to get from one conductor to the other. Like using a small diameter chain link in-line to join two big chains together. It will work, but you restrict current capacity. In actual use, it acts like an inline resistor, and will likely get warm/hot. Split bolts are ugly, but they bond both conductors directly together and little current goes through the bolt, there is no current capacity loss if the splice is tight.


    This is one of the "correct" in-line ways to do it :

    https://www.amazon.com/Easy-Splice-L.../dp/B008KMKESI

    No cross-sectional loss with a splice like this. You can then heat shrink it.
    Yeah,I did some calculating of cross sectional areas and you’re right.
    I wonder if I could solder cables in tube in such a way that space between cable ends
    was filled with solder, conducting current between the ends.
    Miller a/c-d/c Thunderbolt XL
    Millermatic 180
    Purox O/A
    Smith Littletorch O/A
    Hobart Champion Elite

  10. #10
    Join Date
    Mar 2015
    Location
    Milwaukee, WI
    Posts
    249

    Re: Soft copper tube for butt splice

    Tweco TS-3040 copper cable splicer:
    http://www.airgas.com/product/Weldin...CABEgKwtfD_BwE

  11. #11
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    916

    Re: Soft copper tube for butt splice

    Quote Originally Posted by jpump5 View Post
    I thought about that. I’d rather have a permanent connection that’s smaller and cheaper.

    Caveman, if OSHA were ever to inspect my home shop, spliced welding cables would probably be
    one of they’re lesser concerns.
    I just wanted to throw that out just in case you were in a shop somewhere, my shop would be in the same boat , I'm sure!
    NRA LIFE MEMBER
    UNITWELD 175 AMP 3 IN1 DC MIG/STICK/TIG
    MIDSTATES 300 AMP AC MACHINE
    GOD BLESS AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  12. #12
    Join Date
    Mar 2017
    Location
    Forest Grove OR
    Posts
    228

    Re: Soft copper tube for butt splice

    Quote Originally Posted by jpump5 View Post
    Yeah,I did some calculating of cross sectional areas and you’re right.
    I wonder if I could solder cables in tube in such a way that space between cable ends
    was filled with solder, conducting current between the ends.
    Just flux it up real well with some copper pipe flux, drill a 1/8" vent hole in the tube where the wires butt, and solder away. Solder won't conduct as well, but you'll have greater overall cross section, so your joint will probably have the same resistance in the end. It also won't ever come loose, so you don't have to crimp the crap out of it, just enough crimp to keep it together.
    Everlast 350 EXT - Thermal Dynamics Cutmaster 52 - Rogue Fabrication M600 xHD tube bender
    Milwaukee 4208 Mag Drill - Shopmaster Eldorado Combo mill/lathe machine with DRO.

  13. #13
    Join Date
    Sep 2015
    Location
    SE Pa
    Posts
    1,289

    Re: Soft copper tube for butt splice

    I’ve done a few times to lengthen cables on buss box welders.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement