    got arc welder out for boy have go on and he asked why we can't put cables on other way rd?
    ie earth clamp on rod holder side and vice versa.
    in theory should work but must be good reason.
    and don't want to just say cos that's how it says it should be done would like to give him proper explanation.

  2. #2
    Join Date
    Apr 2006
    Location
    Soda springs,Id
    Posts
    4,327

    Re: stick welding q from 10 yr old.

    If it's an AC only welder it doesn't make any difference. An AC/DC set on DC or DC only welder some rods only weld well with a particular polarity.
    Mike
    Ol' Stonebreaker
    "Experience is the name everyone gives to their mistakes"

    Miller 175 mig
    Miller thunderbolt ac/dc stick
    Victor O/A setup
    Makita chop saw

  3. #3
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    5,019

    Re: stick welding q from 10 yr old.

    We want most of the heat at the end of the rod for most DC stick processes. Electrons flow the direction of most of the heat. The rod tip either liquefies, or vaporizes. The exponential expansion of steel as it converts, along with vaporization of flux causes a jetting action blasting metal, and gas at the joint.

    In thin steel with tight fit up using 6013 you might prefer DC straight polarity or DCEN, or DC-. This gives slower deposition.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  4. #4
    Join Date
    Jul 2011
    Location
    Bossier Parish La.
    Posts
    5,286

    Re: stick welding q from 10 yr old.

    Quote Originally Posted by mickg View Post
    got arc welder out for boy have go on and he asked why we can't put cables on other way rd?
    ie earth clamp on rod holder side and vice versa.
    in theory should work but must be good reason.
    and don't want to just say cos that's how it says it should be done would like to give him proper explanation.
    If it's a DC machine, you can point out the DCEP/DCEN switch and tell him that the switch effectively does that for you without having to change the position of the leads. If you change the leads to the way he was asking about, then the DCEP/DCEN switch will become a DCEN/DCEP switch because the label is now in a reverse configuration. One post is positive and the other is negative, flip the switch and the first one is now negative and the other is positive. That should be a simple enough explanation of it for him to understand(maybe).

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement