    Quit welding today. It runs, feeds wire, but won’t arc. I did some research and it sounds as if the contactor may be bad. I cannot hear it slamming shut when I pull the trigger. Any recommendations as far as troubleshooting? I don’t want to replace it if it’s not the problem. Any other things I should check that might cause the problem?

    Thanks,
    Matt


    Sent from my iPhone using Tapatalk
    Matthew Morton
    Texas A&M '06
    Logsdon Seminary '13

    "Who Dares Wins"
    "AFTF"
    "WH2PH"

    SA 200 (Code: 5337)
    TB 302
    CP 302 w/22A Wire Feeder
    MillerMatic 200
    Miller Syncrowave 200
    MillerMatic 252
    BurnTables 4x4 CNC Machine
    Hypertherm 65

  2. #2
    Join Date
    Mar 2014
    Posts
    170

    Re: Millermatic Pulser Quit Welding

    Check for 24v AC at the contactor coil when the gun trigger is pressed. If you have 24v AC there, then run about 6" of wire out of the gun and touch the metal or ground clamp and hold it there. Next take a insulated screwdriver and press in on the spring-activated part of the contactor. If the wire arcs then your contactor is bad. Report back what you find.

  3. #3
    Join Date
    Aug 2011
    Location
    Texas
    Posts
    86

    Re: Millermatic Pulser Quit Welding

    Well, I finally got around to checking things out. I think it was the contractor. Ordered the part and installed it last week. Seems to have fixed the problem. Welds fine now! Hoping I didn't jinx myself!

    Thanks!!
    Matthew Morton
    Texas A&M '06
    Logsdon Seminary '13

    "Who Dares Wins"
    "AFTF"
    "WH2PH"

    SA 200 (Code: 5337)
    TB 302
    CP 302 w/22A Wire Feeder
    MillerMatic 200
    Miller Syncrowave 200
    MillerMatic 252
    BurnTables 4x4 CNC Machine
    Hypertherm 65

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement