    My grandson has a 2001 Pipeliner 200g that the ocv keep dropping out. I will work fine and then it just begans to drop can anyone tell what I need to be looking for. Or have any of you had issues with it. He is wanting to start a new job he is trying to break out to weld pipe and he bought the machine from someone who said it was good. Like some of us when we are young just buy on impulse and now he has a machine that has issues.

    I have only been in production in Rail Road Cars, now work at a depot and welding different platforms. So I have never had any experience with troubling shooting portable machines.

  2. #2
    Join Date
    Nov 2012
    Location
    ROCKVILLE ,,VA
    Posts
    396

    Re: Pipeliiner 200G issues

    check brushes make sure move freely in holder will be start

  3. #3

    Re: Pipeliiner 200G issues

    thanks will start there.

  4. #4

    Re: Pipeliiner 200G issues

    What would you suggest next brushes are ok

  5. #5
    Join Date
    Jul 2012
    Posts
    613

    Re: Pipeliiner 200G issues

    Check trouble shooting section in owners manual :

    https://www.lincolnelectric.com/asse...oln3/im698.pdf

  6. #6
    Join Date
    Nov 2012
    Location
    ROCKVILLE ,,VA
    Posts
    396

    Re: Pipeliiner 200G issues

    next thing come to mind would be engine speed ., from quaijilloweld03 manual he sent ,,need run constant 1600 rpm at
    welding load speed so can check with rpm gage see what getting? me sa 200 dude,, would adjust governor and carb ,, not familiar with this newer machine,,, but another thing check be idler solenoid see if in bind (dirt) ? not releasing full engine speed

  7. #7

    Re: Pipeliiner 200G issues

    Grandson decided to sell he is on his way to South Carolina going to try to pick up a SA there thanks for all of your suggestions. Looks like he will be the helper on this job.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement