    Picked up this metal table for $35,I plan on using it as a weld table/work bench.my question is its been painted so should I clean the top off and remove all the paint or just leave it?As you can see its chipped and already has some bare metal showing.

    Sent from my SM-N950U using Tapatalk

  2. #2
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    1,566

    Re: New welding table question

    Run a flap disc over the top to ensure a good ground all over. Then a very light coat of oil will prevent rust.

    I occasionally run a disc on mine to clean up any rust and BB’s.

    Paint on the legs is fine.
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211 w/Spoolmate
    Miller 375 Plasma Cutter
    Miller Thunderbolt XL AC/DC
    Hobart Handler 120

    10FtDrillBit.com

  3. #3
    Join Date
    Aug 2018
    Posts
    21

    Re: New welding table question

    Thats what i pretty much figured I should do,but i wanted to verify with the experts. I say for $35 I didn't do to bad. Heck i could probably turn around and sell it for a couple hundred.

    Sent from my SM-N950U using Tapatalk

  4. #4
    Join Date
    Jun 2012
    Location
    CT
    Posts
    3,322

    Re: New welding table question

    Paint on the legs may not be OK if you plan on clamping your ground clamp there. Wherever you plan on doing that, make sure you get the paint off. Not the whole leg, just the area where you want to put the clamp.
    Millermatic 252
    Syncrowave 250
    Purox Metalmaster

  5. #5
    Join Date
    Aug 2018
    Posts
    21

    Re: New welding table question

    Got it done and put a coat of wd40 on thd top. Here's a before, during and finished picture.

    Sent from my SM-N950U using Tapatalk

  6. #6
    Join Date
    Jun 2012
    Location
    CT
    Posts
    3,322

    Re: New welding table question

    Looks nice...how flat and how thick is the top, just out of curiosity. I use Break Free CLP on my table top and my guns. keeps rust away pretty well.
    Millermatic 252
    Syncrowave 250
    Purox Metalmaster

  7. #7
    Join Date
    Aug 2018
    Posts
    21

    Re: New welding table question

    To be honest i never measured the thickness.If i had to guess maybe 3/8 thickness.

    Sent from my SM-N950U using Tapatalk

  8. #8
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    1,566

    Re: New welding table question

    Good point about the paint on the legs. I would drill a hole in the legs or frame and put a 3/8” bolt with jam nut outside and lock nut inside. Then use that for a ground point. That’s how my table is.

    Good score on the table! You couldn’t build it for twice that.
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211 w/Spoolmate
    Miller 375 Plasma Cutter
    Miller Thunderbolt XL AC/DC
    Hobart Handler 120

    10FtDrillBit.com

  9. #9
    Join Date
    Aug 2018
    Posts
    21

    Re: New welding table question

    Thanks!when i saw it on facebook marketplace I knew I had to jump on it. I hit the whole table with a wire wheel,then the top with a flapper wheel and one part of the frame for a ground.also mounted a vise on one corner.

    Sent from my SM-N950U using Tapatalk

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement