    Are you familiar with Swagelok? Proprietary compression fittings, you can for sure get a compression x JIC fitting that will work.

  2. #27
    Join Date
    Feb 2015
    Posts
    29

    Re: TIG hydraulic fittings.......weld or braze?

    Are you familiar with Swagelok? It is proprietary compression fittings. I am fairly certain that they can supply a tube compression x JIC fitting that will work for you. There's probably a vendor near you. No affiliation, BTW.