    hello there

    I am wondering if there is some way to adjust the 'arc force' on a miller dynasty when using HF tig...

    it's like the machine I'm using has ridiculous penetration from 3/9 to 12 while other machines the weld metal sits where you put it

    I'd like to turn this penetration down if I could

    anyway.. ty in advance for reading and commenting.. greatly appreciated

  2. #2
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    8,878

    Re: Miller dynasty HF tig arc control?

    I have no clue what you mean.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Th ermalArc400GTSW,LincolnSW2002ea., MillerMatic350P,MillerMatic200withspoolgun,MKCobra Mig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig3ea.

  3. #3
    Join Date
    Feb 2014
    Location
    n.w. of chicago
    Posts
    585

    Re: Miller dynasty HF tig arc control?

    Quote Originally Posted by shovelon View Post
    I have no clue what you mean.
    ditto

  4. #4
    Join Date
    Mar 2018
    Location
    Tampa, Florida
    Posts
    669

    Re: Miller dynasty HF tig arc control?

    Quote Originally Posted by then3wguy View Post
    hello there

    I am wondering if there is some way to adjust the 'arc force' on a miller dynasty when using HF tig...

    it's like the machine I'm using has ridiculous penetration from 3/9 to 12 while other machines the weld metal sits where you put it

    I'd like to turn this penetration down if I could

    anyway.. ty in advance for reading and commenting.. greatly appreciated
    Hi thewguy,

    To avoid getting responses like the above, especially on TIG related questions please furnish as much info as you can, Including.

    Welder model/year
    Polarity
    Amperage(mention if you’re using an amperage controller like a pedal, switch, or tig button)
    Shielding gas used, and flow rate.(Including post/pre-flow Times)
    Tungsten type, diameter, and tip profile.
    Material you’re welding/ Thickness
    Filler, and diameter you’re using.

    Your original question and statement are a little vague, and TIG has lots of variables to be considered when trouble shooting. Instead of trying to take wild stabs in the dark as to what the issue might be, get back to us first with the above information and we should be able to help you.
    Last edited by Mmock4; 09-10-2018 at 06:39 AM.
    -Mark Smith

    Vulcan ProTig200
    Vulcan MigMax215

    Everlast PowerArc 210STL
    Hypertherm PowerMax45 Xp

  5. #5
    Join Date
    Jul 2008
    Location
    Long Island
    Posts
    2,911

    Re: Miller dynasty HF tig arc control?

    Arc force is a stick feature. Miller calls it “dig”. Refer to your manual.

    And on TIG, if you’re getting too much penetration, either turn the amps down or move faster.

  6. #6
    Join Date
    Jul 2007
    Location
    Lake Of The Ozarks MO
    Posts
    280

    Re: Miller dynasty HF tig arc control?

    Well since the OP hasn't returned I'll take a "wild stab" at it.
    The Dynasty is an inverter. Inverter arc is quite different than an old transformer style machine's arc.

    The old school machine, esp. with a balled tungsten tends to make a wider arc. When you begin a puddle, many times it begins or forms (melting) at the outside (of the puddle) and then works it's way inward.
    The new school machine begins at the center and works outward.
    I had at one time an AB/P 330 and a Dynasty 200. Once I determined that (puddle thing) I became more accustomed to that style of arc. Then I preferred it, so I got a bigger Dynasty. I should have kept the 330 but I needed the money then. (still do)

    That is my take on it. YMMV. HTH
    Miller Dynasty 700
    Miller 350P with Aluma-pro push-pull
    Miller 280 Dynasty with expansion card
    Dynasty 200 DX
    MigMax 215


    Enuff power and hand tools to create one of anything..... but mass produce nothing!!!

  7. #7
    Join Date
    Feb 2010
    Location
    Northern MN
    Posts
    1,287

    Re: Miller dynasty HF tig arc control?

    If you're welding in AC you can adjust the frequency, wave form, AC balance, time at peak, and about a dozen other parameters that will effect the arc. If you want it to weld like an old tranformer, set it 60Hz and 50/50 balance with a sine wave.

    Now for DC, you're stuck with polarity, amperage, tungsten tip shape. The rest is up to you.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement