    Quick question from the group here... btw I did try to search but probably didn't type the correct question.

    I am going to build a several signs made from 1-1/4" x 1/8" sq tube that will be 22' long. In the past I splice 6061 tube together to get the length but I am thinking about using 6063 for the long pieces and 6061 for the shorter ones. The processes used will be pulse mig with 4043 filler and tig with 5356. My brain tells me that there is no problem welding the two alloys together but I haven't done that in the past so I'm asking if there is anything I should avoid here? The parts will not be anodized so I'm not concerned about that.

    Thanks everyone

  2. #2
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    8,877

    Re: Welding 6061 to 6063

    No problem at all. Welding the two is done quite regularly.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Th ermalArc400GTSW,LincolnSW2002ea., MillerMatic350P,MillerMatic200withspoolgun,MKCobra Mig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig3ea.

  3. #3
    Join Date
    Sep 2016
    Location
    Near Traverse City, Mi.
    Posts
    262

    Re: Welding 6061 to 6063

    I did it for a boarding ladder for a boat. Either the flats or the tube was 6061, the other was 6063. I used 5356. Has lasted fine with a 350 lb guy going up and down it every day on his live aboard. I am not a welder or metalurgist. Just a hack with a boat shop...
    Miller Dynasty 280 DX, Lincoln 210 MP

  4. #4
    Join Date
    Jun 2005
    Location
    La Verne Ca.
    Posts
    215

    Re: Welding 6061 to 6063

    Thanks guys!!!

  5. #5
    Join Date
    Oct 2009
    Location
    Cartersville, Georgia
    Posts
    358

    Re: Welding 6061 to 6063

    Have you checked on 24' lengths? They are common as dirt over here.
    Who is John Galt?

  6. #6
    Join Date
    Jun 2005
    Location
    La Verne Ca.
    Posts
    215

    Re: Welding 6061 to 6063

    Are you getting 6061 in 24'?
    My supplier has 6061 only in 20' but 6063 comes 24'.

  7. #7
    Join Date
    Oct 2009
    Location
    Cartersville, Georgia
    Posts
    358

    Re: Welding 6061 to 6063

    Quote Originally Posted by KGIOR View Post
    Are you getting 6061 in 24'?
    My supplier has 6061 only in 20' but 6063 comes 24'.
    I definitely have bought 24' lengths of 3/4 square, 1" square and 1 1/2" square in 6061 in the last year or so. I couldn't find the last time I bought 1 1/4, to see if they were also 6061.

    From one distributor, 6061 square is primarily 24' sticks, and 6063 square is usually 21' 1".
    From another, they primarily stock 24' sticks of both alloys, but have a more limited selection of 6061 square tube. A true 20' is actually a rarity in square tube for me.
    Last edited by bassboy1; 09-13-2018 at 06:09 PM.
    Who is John Galt?

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement