    First time here,

    Some one at work gave me a spool gun that they ran on a Powcon 300SM. I purchased a Powcon 300sm from a surpluser. It was wired and used on 230 volt 3 phase. After getting it home. I hooked it up 230 volt single phase. I did so after reading several Posts. The led and the fan runs strong but can get any current to weld with. I plugged the spool gun in and pulled the trigger. it spools the wire but no current. Would anyone have any trouble shooting advice?

    Thanks,

    Mek

  2. #2
    Join Date
    Dec 2011
    Location
    Tampa FL
    Posts
    994

    Re: Powcon 300SM

    Did you connect the black and white wires and cap off the red wire? Did you verify the arrangement of the internal jumpers?

    https://arconweld.com/custom/Powcon_...1C%20300SM.pdf
    Mike

  3. #3
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    1,421

    Re: Powcon 300SM

    Welcome!
    NRA LIFE MEMBER
    UNITWELD 175 AMP 3 IN1 DC MIG/STICK/TIG
    MIDSTATES 300 AMP AC MACHINE
    GOD BLESS AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  4. #4
    Join Date
    Sep 2018
    Location
    Chamberlain, South Dakota
    Posts
    2

    Re: Powcon 300SM

    Thank you for responding Mike,

    The welder came with a cord attached I just had to put a 50 amp plug on. At that process I cut the red wire short and just hooked the black and the white to the 2 legs. Name:  230 volt connect.JPG
Views: 19
Size:  37.7 KB after reading the book it looked like it was wired for 230 volt which my shop is 240 volt single phase.

    any ideas??

    Thanks,

    Mark

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement