  1. #1

    68 Sa200 Need major help Gen Sparking

    68 Sa200 Need major help

    Hi, i have a old 1968 sa200

    the welder does run and strike a arc but i noticed that here is some major arcing going on in the main gen area
    i took the shield off and its looks like its coming from the brushes.. i checked all the brushes and they seem to be in good
    shape and they're all free not hanging up.

    the welder does Idle up when i strike a arc but the gen arcs really bad. not sure what to do at this point

    please help me thanks again

    Mike

  2. #2

    Re: 68 Sa200 Need major help Gen Sparking

    Hi guys i am new to the site. sorry if i posted the help question in the wrong section.
    i am auto mechanic by trade so i do have some Knowledge of welders and how they work but his one has me stumped.


    Mike

  3. #3
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,037

    Re: 68 Sa200 Need major help Gen Sparking

    From the photo you sent me the armature has a short causing that damage to the commutator bars. Gonna need a replacement or rewind.

    Name:  20181108_173638.jpg
Views: 44
Size:  116.5 KB
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  4. #4
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,037

    Re: 68 Sa200 Need major help Gen Sparking

    Mind sharing your general location?
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  5. #5

    Re: 68 Sa200 Need major help Gen Sparking

    Hi i am up near edmonton alberta canada where would i take the armature to get fix i can remove it ? or can i get a replacement ?

    Mike

  6. #6
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,037

    Re: 68 Sa200 Need major help Gen Sparking

    Rewinds are expensive. Here's one example from the rewinder I use:
    http://eurtonelectric.com/catalog/ar...rmature_Rewind
    Located in CA shipping adds to the figure.

    You may be fortunate to find a parts unit in or close to your area with a good replacement.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement