Welding a atv rear axle to its ring gear
RSS | Subscribe | Contact Us | Advertise | About Us
Page 1 of 2 12 LastLast
Results 1 to 25 of 30
  1. #1

    Welding a atv rear axle to its ring gear

    Hi I would like to stick weld my axle on my atv to the ring gear it is slipping, any suggestions about rods etc

  2. #2
    Join Date
    Jun 2007
    Posts
    197

    Re: Welding a atv rear axle to its ring gear

    Ni-cads... Nickle rods any time that you weld hard or two different kind of steel together.

  3. #3
    Join Date
    Jan 2009
    Location
    North Chili N.Y.
    Posts
    307

    Re: Welding a atv rear axle to its ring gear

    It will take the heat treat out of the gear.

  4. #4
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    4,052

    Re: Welding a atv rear axle to its ring gear

    TIG brazing would be lees heat...

  5. #5
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    9,259

    Re: Welding a atv rear axle to its ring gear

    Er312 is your friend. Lincoln used to sell it as their "All Purpose Maintainance Filler". You can also find it now labeled as "SuperMissileWeld".

    I use it on gears and bearings. The high ferrite content and fast freeze attributes help prevent cracking. Tensile is above 100ksi which is a better match to the gears. You can find it as Tig filler or stick electrodes.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Th ermalArc400GTSW,LincolnSW2002ea., MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig4ea,MigMax1ea.

  6. #6

    Re: Welding a atv rear axle to its ring gear

    Thank you I thought it would be different welding the too parts together I will read up on the nickel rods
    This is where I want to weld the housing slides over it so if it doesn't work or it breaks I can take it apart
    Name:  IMG_4393.jpg
Views: 692
Size:  58.6 KB

  7. #7

    Re: Welding a atv rear axle to its ring gear

    Thank you I will try to find out about er312 rods

  8. #8
    Join Date
    Dec 2009
    Location
    Stevens Point, WI
    Posts
    5,003

    Re: Welding a atv rear axle to its ring gear

    Good advise to follow. Should weld up nice and away from the teeth. have at'er
    12v battery, jumper cables, and a 6013.
    I only have a facebook page. https://www.facebook.com/pages/VPT/244788508917829

  9. #9

    Re: Welding a atv rear axle to its ring gear

    Quote Originally Posted by VPT View Post
    Good advise to follow. Should weld up nice and away from the teeth. have at'er
    Which rod would you use

  10. #10

    Re: Welding a atv rear axle to its ring gear

    How could I figure out what metal the parts are

  11. #11
    Join Date
    Jan 2004
    Location
    Northern Cal., Shasta County
    Posts
    9,292

    Re: Welding a atv rear axle to its ring gear

    A lot of axle material and even the gears have a teeny bit of vanadium. Increases toughness and corrosion resistance. Do a search with 'axles crankshafts vanadium' .. Don't know that an atv would warrant a more expensive alloy but still it is pretty much standard practice.
    "The things that will destroy America are prosperity at any price, peace at any price, safety first instead of duty first, the love of soft living and the get rich quick theory of life." -Theodore Roosevelt

  12. #12
    Join Date
    Mar 2009
    Location
    MN
    Posts
    5,159

    Re: Welding a atv rear axle to its ring gear

    Id be worried about the axle wanting to break at the weld if that's a one piece axle like on a sport model.
    My name's not Jim....

  13. #13
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    2,425

    Re: Welding a atv rear axle to its ring gear

    I think I would do a couple of good tacksmaybe 1/4 to 1/2' long 180* apart.
    NRA LIFE MEMBER
    UNITWELD 175 AMP 3 IN1 DC MIG/STICK/TIG
    MIDSTATES 300 AMP AC MACHINE
    GOD BLESS AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  14. #14
    Join Date
    Dec 2009
    Location
    Stevens Point, WI
    Posts
    5,003

    Re: Welding a atv rear axle to its ring gear

    Quote Originally Posted by Buzzboxer View Post
    Which rod would you use
    The mentioned er312 or, since I have them on hand, I would use er308l, either will get the job done. Just don't cook the axle to much.
    12v battery, jumper cables, and a 6013.
    I only have a facebook page. https://www.facebook.com/pages/VPT/244788508917829

  15. #15
    Join Date
    Jul 2008
    Posts
    2,224

    Re: Welding a atv rear axle to its ring gear

    Quote Originally Posted by CAVEMANN View Post
    I think I would do a couple of good tacksmaybe 1/4 to 1/2' long 180* apart.
    +1

    Probably don't need much.

    Also, if I didn't have any super duper NASA missileweld, I'd probably use 7018, cross my fingers, and call it macaroni. I've gotten away with a lot of things I probably shouldn't have with 7018.
    Last edited by Kelvin; 11-11-2018 at 08:53 PM.

  16. #16
    Join Date
    Dec 2009
    Location
    Stevens Point, WI
    Posts
    5,003

    Re: Welding a atv rear axle to its ring gear

    can't delete post, been drinking....
    12v battery, jumper cables, and a 6013.
    I only have a facebook page. https://www.facebook.com/pages/VPT/244788508917829

  17. #17

    Re: Welding a atv rear axle to its ring gear

    Would you do a couple of tacks or weld all the way around? Does it need to be heated first ?
    Last edited by Buzzboxer; 11-11-2018 at 10:41 PM. Reason: Adding to post

  18. #18
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    2,425

    Re: Welding a atv rear axle to its ring gear

    I would do a couple of tacks, this will minimize heat input which will help with warping
    , the gear at least will have some heat treatment and the axle as well, if you don't know what you are doing then preheating may affect the heat treat. a couple of tacks with the 312, quick & easy, don't overthink it, make sure you get it cleaned of the gear oil, whatever you do, DON'T USE A CHLORINATED SOLVENT OF ANY KIND, you can use non chlorinated brake cleaner, spray carburetor/fuel injector/throttle body cleaner etc. I think the key is to minimize heat input, thus the 2 tacks, the first tack is going to try to pull the axle, and the second will pull it back, hopefully the gear is not sloppy loose on the shaft, if it is then maybe 4 tacks working to make sure the gear is straight and the backlash is right. Honestly I think 2-4 1/4" tacks will be just fine. Lotsa folks tend to overweld things like this.
    NRA LIFE MEMBER
    UNITWELD 175 AMP 3 IN1 DC MIG/STICK/TIG
    MIDSTATES 300 AMP AC MACHINE
    GOD BLESS AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  19. #19

    Re: Welding a atv rear axle to its ring gear

    I have tried to find the er312 stick welding rods but I can't seem to find them even online any idea where to get them?

  20. #20
    Join Date
    May 2018
    Location
    the Netherlands
    Posts
    172

    Re: Welding a atv rear axle to its ring gear

    Quote Originally Posted by Buzzboxer View Post
    I have tried to find the er312 stick welding rods but I can't seem to find them even online any idea where to get them?
    Try searching for 312L-16.

    https://store.cyberweld.com/hobart-3...80630-rdp.html

    https://www.ebay.com/itm/Stainless-S...-/323155709819

    Certanium 707SP is also 312L-16 as far as I know but very expencive.

    https://www.lawsonproducts.com/Certa...rode/P12610.lp

    And the Super Missileweld Shovelon mentioned.

    http://www.harrisproductsgroup.com/e...ssileweld.aspx

    https://www.netwelder.com/harris-sup...18-electrodes/

    http://www.airgas.com/product/Weldin...y/p/HARULSMW60


    In Europe Lincoln has the Limarosta 312 but I can't find that one on the Lincoln USA site.
    I have 312L-16 rods from Lastek, but those are probably not available in the USA.

    If You really can't get some 312 rods, 309 will do it.
    Last edited by E T; 11-12-2018 at 02:49 PM.
    Kemppi minarc 150
    Esab powercut 400

  21. #21

    Re: Welding a atv rear axle to its ring gear

    hey, it seems like not a big, but a strong weld is needed for the first time only. then you can notice the performance and optimize how good it is performing. if you still hear those noises or whistles, do not ignore that alarm if you don't want to cause it to your life. Take is to an axle repair service to be maintained easily and properly.

  22. #22
    Join Date
    Dec 2018
    Posts
    1,802

    Re: Welding a atv rear axle to its ring gear

    Never seen an atv axle. Do they just stick out like a stub, or are they supported at the outboard end by a bearing?

  23. #23
    Join Date
    Dec 2018
    Posts
    1,802

    Re: Welding a atv rear axle to its ring gear

    Name:  MjAxMzM4Mg-8ad61daf.jpg
Views: 340
Size:  84.8 KB

    Like this?????????????

    How in the smurf does the axle fit the ring gear......press fit?

  24. #24
    Join Date
    Dec 2018
    Posts
    1,802

    Re: Welding a atv rear axle to its ring gear

    No differential????????????? I'm all confuseled

  25. #25
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    4,052

    Re: Welding a atv rear axle to its ring gear

    Quote Originally Posted by farmersammm View Post
    No differential????????????? I'm all confuseled
    Most all the {atv's} have solid axles on the rear, this is why they sell so many tires for them

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  