    Welding Magnet Demagnetized??

    Ok so I stepped on the cheap sheet metal ground clamp that came with my machine and it broke. So I took apart an old HDD, salvaged the magnet from that and used that as a magnet as a diy mag. ground clamp. After 15min of welding, the magnet is barely sticking to metal, UPDATE (it's been now completely Demagnetized) when I pulled it out of the HDD it could like 10lbs. Did the electricity or the heat mess it up, how's that possible. If so, I'd imagine the store bought mag clamps will fail after a while like mine. Lol??
    Last edited by n00b; 11-09-2018 at 08:37 PM.
    "It's always SPOOOOOOKY Season."

    NJ- "Its only illegal if you get caught" - Chinesium welder

    Yoda: Overlord of Magic Smoke, I am

  2. #2
    Join Date
    Mar 2017
    Location
    bar stool
    Posts
    2,097

    Re: Welding Magnet Demagnetized??

    Memo: Heat destroys magnetic fields.

    Might by why blacksmiths often use a magnet to determine when their heat is at correct temperature.

  3. #3
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    2,225

    Re: Welding Magnet Demagnetized??

    Dropping a magnet will weaken it as well. Did it get hot because the ground was close to your welding or because the surface was dirty and a poor connection? I've had a cheap commercial one on my handle for about a year with no problems, but I actually use it more to hang the clamp on the side of my bench when I'm not using it than as a ground.
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  4. #4
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    4,165

    Re: Welding Magnet Demagnetized??

    Quote Originally Posted by n00b View Post
    .. If so, I'd imagine the store bought mag clamps will fail after a while like mine. Lol??
    Your imagination would be wrong. I've had mine for years. a few actually.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.


  5. #5
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    2,335

    Re: Welding Magnet Demagnetized??

    Hard drive magnets are rare earth.... rare earth magnets can only handle so much heat...


    https://www.kjmagnetics.com/blog.asp...dymium-magnets


    And passing heavy currents directly though them is probably worse than direct heat as the 'skin' of the magnet is much a better conductor than the innards.

  6. #6
    Join Date
    Oct 2009
    Location
    Austin TX
    Posts
    818

    Re: Welding Magnet Demagnetized??

    I was thinking that you might be welding with AC, which could confuse the magic elves in the magnet and end up degaussing it.
    Miller Syncrowave 350
    Millermatic 252/ 30A spoolgun
    Miller Bobcat 225g w/ 3545 spoolgun
    Lincoln PowerArc4000
    Lincoln 175 Mig
    Lincoln 135 Mig
    Everlast 250EX Tig
    Century ac/dc 230 amp stick
    Victor O/A
    Hypertherm 1000 plasma

  7. #7
    Join Date
    Jun 2016
    Location
    Not there
    Posts
    3,324

    Re: Welding Magnet Demagnetized??

    Magnets are for holding for tacking. PERIOD

  8. #8
    Join Date
    Jul 2008
    Posts
    1,950

    Re: Welding Magnet Demagnetized??

    Quote Originally Posted by Bonzoo View Post
    Magnets are for holding for tacking. PERIOD
    Don't forget "and causing arc blow"

  9. #9
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    2,335

    Re: Welding Magnet Demagnetized??

    Quote Originally Posted by Kelvin View Post
    Don't forget "and causing arc blow"
    ^^ THIS!!


    I find them particularly useful for creating different visual effects to make my welds look more like someone else did them

  10. #10
    Join Date
    Apr 2018
    Posts
    119

    Re: Welding Magnet Demagnetized??

    Yeah I got confused b/c as the magnet died the rod didn’t arc, the magnet did, I was like WTF is that.
    "It's always SPOOOOOOKY Season."

    NJ- "Its only illegal if you get caught" - Chinesium welder

    Yoda: Overlord of Magic Smoke, I am

  11. #11
    Join Date
    Jul 2014
    Location
    Bulldog Heaven at the end of my chain
    Posts
    3,743

    Re: Welding Magnet Demagnetized??

    Quote Originally Posted by ronsii View Post
    ^^ THIS!!


    I find them particularly useful for creating different visual effects to make my welds look more like someone else did them
    Yup, like teaching my seven year old granddaughter to stick weld right?????
    Slob

    Purveyor of intimate unparalleled knowledge of nothing about everything.

    Oh yeah, also an unabashed internet "Troll" too.....

  12. #12
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    2,335

    Re: Welding Magnet Demagnetized??

    Quote Originally Posted by n00b View Post
    Yeah I got confused b/c as the magnet died the rod didn’t arc, the magnet did, I was like WTF is that.
    So now all you got to do is get a good powerful straight polarity electromagnet(used MRI machine...) then heat the dead magnet up past curie temp and remagnetize it

  13. #13
    Join Date
    Mar 2017
    Location
    bar stool
    Posts
    2,097

    Re: Welding Magnet Demagnetized??

    If you want a real fun show try cutting a ceramic magnet or even carbide cutter with the plasma machine.

  14. #14
    Join Date
    Jul 2014
    Location
    Bulldog Heaven at the end of my chain
    Posts
    3,743

    Re: Welding Magnet Demagnetized??

    Quote Originally Posted by Virgil5 View Post
    If you want a real fun show try cutting a ceramic magnet or even carbide cutter with the plasma machine.
    I've only seen that once in a video. That was enough of an education to not try it myself.

    Always used a diamond wheel myself, ($$$).
    Slob

    Purveyor of intimate unparalleled knowledge of nothing about everything.

    Oh yeah, also an unabashed internet "Troll" too.....

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement