    I have a Miller 330 a/bp that's not running at full capacity I'm only getting about 250 amps out at the highest setting. I have it on a 60 amp breaker which I know isn't large enough but it doesn't even trip that. I have checked the taps and it looks like they are set to 220. Where's the next area I should be looking? I would like the higher amperages so I can use it to gouge. Thanks.

    Sent from my Pixel 2 using Tapatalk

  2. #2

    Re: Miller 330 a/bp

    The easy thing to do is to check the copper contacts on the range switch. Make sure they're clean and making good contact. Are you using a pedal? There might be a fault in that. There might be a problem with one of the rectifiers.

    See this thread:
    https://forum.millerwelds.com/forum/...miller-330a-bp

  3. #3
    Join Date
    Aug 2013
    Location
    Caledonia Mn
    Posts
    45

    Re: Miller 330 a/bp

    Quote Originally Posted by PaulAm View Post
    The easy thing to do is to check the copper contacts on the range switch. Make sure they're clean and making good contact. Are you using a pedal? There might be a fault in that. There might be a problem with one of the rectifiers.

    See this thread:
    https://forum.millerwelds.com/forum/...miller-330a-bp
    No pedel just stick welding. I'll have to check the diodes and rectifiers and maybe give miller tech support a call. Maybe work the range lever back and forth.

    Sent from my Pixel 2 using Tapatalk

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement