    Welding Chrome Vanadium Coated Wrench

    I have a metal art project in mind and will use a chrome vanadium coated wrench as part of it. Have no clue how to weld it to mild steel parts. What process should I use. Have MIG and TIG. Should I just grind off the coating where I want the welds to be and then weld as normal, as I assume the base metal is carbon steel. Thanks for your help.

  2. #2
    Join Date
    Jul 2014
    Location
    Bulldog Heaven at the end of my chain
    Posts
    3,743

    Re: Welding Chrome Vanadium Coated Wrench

    Quote Originally Posted by John Sundquist View Post
    I have a metal art project in mind and will use a chrome vanadium coated wrench as part of it. Have no clue how to weld it to mild steel parts. What process should I use. Have MIG and TIG. Should I just grind off the coating where I want the welds to be and then weld as normal, as I assume the base metal is carbon steel. Thanks for your help.
    Vanadium and chromium are alloying components of the steel the wrench is made from, chromium is also the bright shiny "coating", or more proper term, "electroplating" process that makes it shiny and corrosion resistant.

    If not for rugged use you can weld it easily conventionally.
    Last edited by Slob; 11-30-2018 at 10:32 AM.
    Slob

    Purveyor of intimate unparalleled knowledge of nothing about everything.

    Oh yeah, also an unabashed internet "Troll" too.....

  3. #3
    Join Date
    Oct 2014
    Posts
    390

    Re: Welding Chrome Vanadium Coated Wrench

    You should have no problem welding it. I actually prefer the way it welds. Not much different really it just seems to make such a nice easy to run puddle for some reason. Tool steel all seems that way to me. Easy to weld nicely.
    Last edited by danielplace; 11-30-2018 at 10:41 AM.

  4. #4
    Join Date
    Nov 2018
    Posts
    13

    Re: Welding Chrome Vanadium Coated Wrench

    If you want the plating removed, soak in white vinegar a few days.


    Sent from my iPhone using Tapatalk

  5. #5
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    9,054

    Re: Welding Chrome Vanadium Coated Wrench

    Quote Originally Posted by John Sundquist View Post
    I have a metal art project in mind and will use a chrome vanadium coated wrench as part of it. Have no clue how to weld it to mild steel parts. What process should I use. Have MIG and TIG. Should I just grind off the coating where I want the welds to be and then weld as normal, as I assume the base metal is carbon steel. Thanks for your help.
    Your plan is sound. I do it that way regularly and use ER312 as filler. https://www.lincolnelectric.com/en-u...ncolnElectric)
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Th ermalArc400GTSW,LincolnSW2002ea., MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig4ea,MigMax1ea.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement