FTT report aws D17.1
RSS | Subscribe | Contact Us | Advertise | About Us
Results 1 to 5 of 5
  1. #1

    FTT report aws D17.1

    Hello all,
    Working on getting an AWS D17.1 job qualified and I just can`t figure out what an FTT report is or if it is relevant to what I am doing.
    Can anyone advise me?

    Thanks!

  2. #2
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    9,054

    Re: FTT report aws D17.1

    That is new to me as well.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Th ermalArc400GTSW,LincolnSW2002ea., MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig4ea,MigMax1ea.

  3. #3
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    9,054

    Re: FTT report aws D17.1

    Ok.

    The consensus is that FTT means Fracture Toughness Test. Or in more common terms Charpy v-Notch test. Apparently AWS is dropping the abbreviation CVN for FTT. Wish they would have clued us in a little better.

    Question now is when is CVN required for the report(most likely not unless engineering requests it in writing). If not just put on the report Not Applicable or N/A.
    Last edited by shovelon; 12-11-2018 at 11:54 AM.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Th ermalArc400GTSW,LincolnSW2002ea., MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig4ea,MigMax1ea.

  4. #4
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,243

    Re: FTT report aws D17.1

    The current aws mag just did an article on charpy-v testing

  5. #5
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    9,054

    Re: FTT report aws D17.1

    I will have to give that a read. Interesting stuff.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Th ermalArc400GTSW,LincolnSW2002ea., MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig4ea,MigMax1ea.

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement