    Re: Help with cold saw please!

    Nice setup.

  2. #27
    Join Date
    Sep 2013
    Posts
    151

    Re: Help with cold saw please!

    Quote Originally Posted by Lis2323 View Post

    I’m done. Locking swivel mechanism works well. I actually surprise myself sometimes.
    That looks great! You’ll be glad you built it every time you use it.

    I think I saw mention of a handle that attaches above the handle on those Makita dry saws to retract the blade guard. Mine doesn’t have one but it seems like it could be handy for lining up to the cut. Anyone have experience with it?



    Sent from my iPhone using Tapatalk

  3. #28
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    1,495

    Re: Help with cold saw please!

    Quote Originally Posted by djd775 View Post
    That looks great! You’ll be glad you built it every time you use it.

    I think I saw mention of a handle that attaches above the handle on those Makita dry saws to retract the blade guard. Mine doesn’t have one but it seems like it could be handy for lining up to the cut. Anyone have experience with it?



    Sent from my iPhone using Tapatalk
    Hmm. That’s interesting. On my saw the moment the handle starts to lower, the blade guard simultaneously retracts to expose the cut line.

    Perhaps the handle is to lift the guard out of the way to easily facilitate a blade change or accessing the arbor bolt?


    Sent from my iPad using Tapatalk
    :

  4. #29
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    8,629

    Re: Help with cold saw please!

    I used a vfd for mine and welcome to the forumName:  DB22F144-C208-4144-93F9-D29C63AA4C4B.jpg
Views: 291
Size:  128.0 KB

  5. #30
    Join Date
    Feb 2014
    Location
    n.w. of chicago
    Posts
    850

    Re: Help with cold saw please!

    Quote Originally Posted by motolife313 View Post
    I used a vfd for mine and welcome to the forumName:  DB22F144-C208-4144-93F9-D29C63AA4C4B.jpg
Views: 291
Size:  128.0 KB
    Nice saw moto but jesus you need a tenuous shot to walk through that tinder box

  6. #31
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    4,288

    Re: Help with cold saw please!

    Quote Originally Posted by Lis2323 View Post
    Hmm. That’s interesting. On my saw the moment the handle starts to lower, the blade guard simultaneously retracts to expose the cut line.

    Perhaps the handle is to lift the guard out of the way to easily facilitate a blade change or accessing the arbor bolt?


    Sent from my iPad using Tapatalk
    Yeah, the guard retracing is really a non issue. I drilled a small hole in the outer guard, thru the inner guard with it fully retracted that I slip a nail or welding rod stub thru for blade changes.
    Miller xmt304, Miller S22 p12, Miier Maxstar SD, Miller 252 w 30A, Miller super32p12, Lincoln Ranger 9, Thermal Arc 181I with spoolgun, Hypertherm 10000 ,Smith torches. Esab 161lts miniarc.

  7. #32
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    1,495

    Re: Help with cold saw please!

    Quote Originally Posted by M J D View Post
    Yeah, the guard retracing is really a non issue. I drilled a small hole in the outer guard, thru the inner guard with it fully retracted that I slip a nail or welding rod stub thru for blade changes.
    Shoot. Good idea. I’ll have to do that!


    Sent from my iPad using Tapatalk
    :

  8. #33
    Join Date
    Sep 2013
    Posts
    151

    Re: Help with cold saw please!

    My blade retracts as soon as I push the saw head down too; but not always far enough to line the blade up easily to the mark...but it can be rolled out if the way farther by hand so you’re right, it’s not a huge deal.

    Biggest issue is if I try to measure off the side of the blade for cut lengths rather than marking the piece...need 3 hands to hold everything so it doesn’t work easily like it does on a bandsaw. My old Ridgid abrasive saw cuts exactly 1” from the edge of the cast base to the side of the blade, so it’s a breeze to clamp pieces at the correct cut location without marking them first. But it’s an abrasive saw, so.....

    Getting back to the Makita dry saw, one thing I do wish for often, is an electric brake. On repetitive cuts you can end up waiting a few seconds for the blade to stop before lining it up to the next mark. Minor issue though, the saw works great.

  9. #34
    Join Date
    Apr 2018
    Location
    Redhook, Brooklyn
    Posts
    4

    Re: Help with cold saw please!

    wow Terry, looks great. thanks so much to everyone for all the input. When the electrician came to hook up the 30 and 50 amp 220, he said the 3 phase would only be another 200$ so I jumped on it and got the Brobo as well. although I cut small stuff, I cut about 3000 cuts a year and plan on about 10,000. Half stainless and half mild up to 3" tube and angle. The saw is a 40/80 rpm. sure hope that is ok. I think the nice thing is that I will be able to cut multiple pieces of the angle at once. That sure will save a ton of time.
    Tarpon, hell yea. but just for fun. usually 10 days a year in the keys. I guide for Striped Bass and Bonito in the New York. that video made me jumpy for april 26th in Key Largo. Thanks a bunch yall. Ill let ya know how the brobo is going
    Brendan

  10. #35
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    8,629

    Re: Help with cold saw please!

    If u get a vfd u can actually slow the rpm to 25 if needed

  11. #36
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    1,495

    Re: Help with cold saw please!

    Good move on the three phase! Made it easy for your decision to buy the Brobo. Certainly the choice I would have made also.

    Post some pics when you are up and cutting!


    Sent from my iPad using Tapatalk
    :

  12. #37
    Join Date
    May 2004
    Location
    Edison Wa.
    Posts
    790

    Re: Help with cold saw please!

    I would be very careful cutting multiple pieces of angle at once.
    The cold saw is very sensitive to the parts vibrating- and if your parts wiggle while the saw blade is in the cut, it can easily crack or break the blade. $150 down the drain just like that.
    I never bundle cut with the cold saw.
    I, or my employees, have broken too many blades.

  13. #38
    Join Date
    Jun 2016
    Location
    Aynor SC
    Posts
    3,947

    Re: Help with cold saw please!

    Quote Originally Posted by Ries View Post
    I would be very careful cutting multiple pieces of angle at once.
    The cold saw is very sensitive to the parts vibrating- and if your parts wiggle while the saw blade is in the cut, it can easily crack or break the blade. $150 down the drain just like that.
    I never bundle cut with the cold saw.
    I, or my employees, have broken too many blades.
    This dude has it ON. If you have a bander, you can band small bundles. It'll help quite a bit

  14. #39
    Join Date
    Jan 2005
    Location
    St. Johns, Michigan
    Posts
    263

    Re: Help with cold saw please!

    Love the little fenders you made Terry!
    Pete




    ESAB SVI300
    ESAB MIG 4 HD
    MILLER PASSPORT 180
    MILLER DYNASTY 300DX
    MILLER COOLMATE 4
    MILLER 30A
    MILLER SPECTRUM 2050
    C&K WF-3
    PrimeWeld Tig 225X

  15. #40
    Join Date
    Jul 2011
    Posts
    790

    Re: Help with cold saw please!

    If that saw is in any kind of decent shape $500.00 for that saw is a great buy. I don’t really even need one and I’d have a hard time passing it up.


    Sent from my iPhone using Tapatalk

  16. #41
    Join Date
    Sep 2013
    Posts
    151

    Re: Help with cold saw please!

    For those of you with experience....how does cold cut compare to dry cut with regard to cut speed, versatility, and blade durability? I have an old Scotchman cold cut that I got real cheap...debating between putting a dry cut motor/blade on the heavy duty base/vise OR getting a vfd or other phase converter and using it as is. I don’t typically need accuracy beyond what my bandsaw and dry cut saw currently offer - speed and practicality are the main considerations for me.


    Sent from my iPhone using Tapatalk

  17. #42
    Join Date
    Jun 2016
    Location
    Aynor SC
    Posts
    3,947

    Re: Help with cold saw please!

    Nice rig. I decided to not use rollers on mine so I just spaced 1" angle, point up. instead.I fount the rollers to be pain when trying to move 1/16 or 1/32. I like the friction of the angle for that. OTOH working with a 15 foot piece of 4 x 4 1/4 wall every day would surely change my tune !.
    I just do ornamental crap. 3 x 3 x 1/8 is "heavy tube" in my world.
    Can't beat that lazy Suzie deal. I've done that for years

  18. #43
    Join Date
    Apr 2018
    Location
    Redhook, Brooklyn
    Posts
    4

    Re: Help with cold saw please!

    Quote Originally Posted by Ries View Post
    I would be very careful cutting multiple pieces of angle at once.
    The cold saw is very sensitive to the parts vibrating- and if your parts wiggle while the saw blade is in the cut, it can easily crack or break the blade. $150 down the drain just like that.
    I never bundle cut with the cold saw.
    I, or my employees, have broken too many blades.

    Thanks for that tech , Reis. All set up for saw and was goo for a minute after new pump, etc. now it is throwing the breaker every time i try to turn it on. I think it is the switch on the saw. the beat goes on!

  19. #44
    Join Date
    Jun 2016
    Location
    Aynor SC
    Posts
    3,947

    Re: Help with cold saw please!

    Absolute. Bundling is for a band saw and buy a metal bander and band it tight. Duct tape wont get it.
    Realistically all toothed saw blades hate vibration. I've byatched at all of them for a Sctotchman type double sided vice. The dont G.A,F. They make more in blades than the saw itself......over time.
    Get some good clamps and get to it.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement