    Hi there,
    I have inherited an old miller bobcat 225. Serial #KJ212853 Stock # 903500. The bottom has rusted thru and the large transformer fell out. I was wondering if anyone would have an idea where the wires from the transformer connect. There is one wire that has stayed intact but the other two have been pulled off there location. If anyone can help in any way I would be very grateful. Thanks!

  2. #2
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,323

    Re: Miller Bobcat 225

    That device in question is either the AC output reactor or DC stabilizer/choke.

    You can get your unit manual here to trace out the leads which will have circuit numbers embossed on them.
    https://www.millerwelds.com/files/ow.../O405D_MIL.pdf

    You can use the parts break-down in the manual to identify which component you're dealing with.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  3. #3
    Join Date
    Sep 2018
    Location
    Cut Off, Louisiana
    Posts
    9

    Re: Miller Bobcat 225

    Thank you Duane,
    Repaired bottom of skid and welded the DC stabilizer back in place. Will be wiring this thing back in proper location and will let you know the outcome. Thanks again and have a nice day!

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement