    I have done a bit of stainless mig welding (mostly just tacking up, and way less then 8 hours total) in my attached garage. Any cutting has been done with a bandsaw, though the parts were also cleaned up with wire wheels and used flap discs.

    Aside from opening the garage door and wearing a 3m 2097 respirator for lung protection, should I be concerned with clothing getting contaminated?

  2. #2
    Join Date
    Oct 2011
    Location
    Hamlin, NY
    Posts
    1,294

    Re: Stainless Steel Safety

    No

    Sent from my LM-Q710.FG using Tapatalk
    Ryan

    Miller Multimatic 200 tig/spool gun/wireless remote
    Millermatic 350P, Bernard/XR Python guns
    Miller Dynasty 350, Coolmate 3.5 & wireless remote
    CK WF1 TIG wire feeder
    Miller Spectrum 375 Xtreme
    Optrel e684
    Miller Digital Elite
    Miller Weld-Mask

  3. #3
    Join Date
    Dec 2008
    Location
    Lockhart,Tx (BBQ capitol of the world)
    Posts
    975

    Re: Stainless Steel Safety

    Contaminated with what?

    Stainless welding is the cleanest welding you will ever do!

  4. #4
    Join Date
    Jun 2016
    Location
    Not there
    Posts
    3,914

    Re: Stainless Steel Safety

    I's be VERY concerned with the clothes being contaminated. By that boleshiit your ol lady gets for soap and fabric softener.
    A lil 304/308/316 dust....might make your ballz itch if it doesnt come out in the spin cycle.
    Good choice of a respirator. The wheel is far worse than the steel

  5. #5
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    9,201

    Re: Stainless Steel Safety

    Quote Originally Posted by Bonzoo View Post
    I's be VERY concerned with the clothes being contaminated. By that boleshiit your ol lady gets for soap and fabric softener.
    A lil 304/308/316 dust....might make your ballz itch if it doesnt come out in the spin cycle.
    Good choice of a respirator. The wheel is far worse than the steel
    Leave your balls it of it. Most probly its that wacky tobacky.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Th ermalArc400GTSW,LincolnSW2002ea., MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig4ea,MigMax1ea.

  6. #6
    Join Date
    Jul 2018
    Location
    Cumbria, UK
    Posts
    470

    Re: Stainless Steel Safety

    I should hope not... most people don't even bother with a respirator while cutting and TIG welding S/S.

    MIG and stick welding S/S is a different ballgame - according to HSE guidelines it puts out a much larger amount of hexavalent chromium than TIG. Should definitely wear a respirator with that. Nasty lung cancer particles.

    Having said that, I've done my share of stick welding stainless and didn't even realise there was an issue until recently.

    http://www.hse.gov.uk/research/rrpdf/rr770.pdf quite a decent bit of unbiased research
    Last edited by Munkul; 03-27-2019 at 03:59 AM.

  7. #7
    Join Date
    Mar 2004
    Location
    B.C. Canada
    Posts
    2,725

    Re: Stainless Steel Safety

    A buddy who was on a large stainless job said that with all the workplace rules it was easier to assume the worst and put everyone on respirators with clean breathing air supply. That was easier than having environmental consultants run up huge charges determining where the stainless dust and fume was a danger. Once you get used to the apparatus you adapt. Some rigs allow you to regulate the temp of the air from warm to cool according to the temp you are working in.

  8. #8
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    8,823

    Re: Stainless Steel Safety

    All that gets contaminated is the wire and disc. Never use a wheel for carbon and then use it for stainless.

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement